MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elix Polymers Elix™ 260 G SAN Polymer Modifier
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; SAN Polymer

Material Notes: High flow SAN copolymer. Used as base resin in color concentrates. Can be blended with high rubber modifiers to manufacture or modify properties profile of ABS 4resin and blends containing Polycarbonate. Improved flow ability for ABS grades. Excellent balance of mechanical properties, process ability and aesthetics. Easy dispersion for pigments and colorants. Physical form: transparent to slightly yellow pellets.

Information provided by Elix Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 50 - 61 g/10 min
@Load 10.0 kg,
Temperature 220 °C
cm³/10 min MVR; ISO 1133
 
Descriptive Properties
Acrylonitrile Content26.5-28.5%lab internal-IR
Base Colormax. 70DIN 6271 (20% solution in DMF)
Residual Styrene< 600 ppmlab internal-GC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elix Polymers ELIX™ 290 G SAN copolymer
Elix Polymers Elix™ 158 I ABS Polymer Modifier
Lotte Advanced Materials Starex® HG-0760GP ABS
INEOS Styrolution Luran® SAN 51 Styrene Acrylonitrile
Elix Polymers Elix™ 280 G SAN Polymer Modifier

PELIX934 / 192528

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.