MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SEKISUI SPI KYDEX® 410 ABS/PVC  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; ABS/PVC Alloy

Material Notes: Proprietary ABS/PVC sheet

KYDEX® 410 is a proprietary ABS/PVC thermoplastic sheet that offers superior thermoformability, rigidity, breakage resistance, chemical resistance and fire retardancy.

KYDEX® 410 is available in a wide range of standard and custom colors, textures, and sheet sizes. It is Underwriters Laboratories, Inc® recognized for UL std 94 V-0, 5V (rating pending).

Applications:

  • Medical Equipment Housings
  • Electrical Equipment Housings
  • Mass Transit Interior Vehicle Components
  • Miscellaneous Applications

Flammability:

  • FAR 25.853a
  • UL94 V-0, 5V @ 1mm
  • Radiant Panel: RP25
  • FMVSS 302

Features:

  • Good for deep or hard to form parts
  • More rigid, parts will deform less when loaded - or can be down-gauged for weight-savings
  • High Notched Izod impact resistance offers resistance to breakage
  • Meets highest standard for chemical resistance for thermoplastic materials
  • Passes UL Std 94 V-0 and 5V in all thicknesses and colors
  • Uniform wall thickness in crisp detail
  • Easy machining and fabricating using conventional methods and equipment
  • Low moisture absorption - no drying needed prior to thermoforming
  • Passes ball pressure test as per UL 60601-1
  • Good low temperature impact resistance

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.29 g/ccASTM D792
Moisture Absorption 0.0700 %
@Temperature 50.0 °C,
Time 86400 sec
After three months storage, drying may be required; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 in/in
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 107ASTM D785
Tensile Strength 53.84 MPaASTM D638
Flexural Strength 76.53 MPaASTM D790
Flexural Modulus 2537 MPaASTM D790
Izod Impact, Notched 94.0 J/m
@Temperature -20.0 °C
ASTM D256
 801 J/m
@Temperature 22.2 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Transverse to Flow 46.0 µin/in-°FASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 160 °FUnannealed; ASTM D648
 175 °FAnnealed at 65.5°C for 8 hrs and cooled slowly; ASTM D648
Flammability, UL94 V-0UL File E115252; Component Recognition
 5VB
@Thickness >=0.991 mm
Underwriters Laboratories., Inc®, File E115252; Component Recognition; UL Standard 94
 
Descriptive Properties
Ball TestPassUL 60601-1, Sub clause 59.2b; Pressure
FlammabilityPassFAR 25.853a; Vertical Burn, 12 sec
 PassFAR 25.853a; Vertical Burn, 60 sec
Motor Vehicle Safety StandardPassFMVSS 302

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SEKISUI SPI KYDEX® 430 ABS/PVC
SEKISUI SPI KYDEX® T-LW Thermoplastic
SEKISUI SPI KYDEX® 100 Polymer Alloy Sheet
SEKISUI SPI KYDEX® FST2 Thermoplastic
SEKISUI SPI KYDEX® 6513 Thermoplastic

PSEKIS028 / 185853

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.