MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Commercial Fine Gold, Wrought then Annealed
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy; Pure Element

Material Notes: Usual purity is 99.95-99.98%. Called proof gold if over 99.99% pure.

Key Words: Gold, Au
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 19.32 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 25
Tensile Strength, Ultimate 130 MPa
Elongation at Break 45 %
Modulus of Elasticity 79.9 GPa
Poissons Ratio 0.42
Shear Modulus 28.1 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000235 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 66.2 J/g
CTE, linear 14.2 µm/m-°C
@Temperature 20.0 °C
 14.6 µm/m-°C
@Temperature 250 °C
 15.2 µm/m-°C
@Temperature 500 °C
 16.7 µm/m-°C
@Temperature 950 °C
Specific Heat Capacity 0.130 J/g-°C
Thermal Conductivity 300 W/m-K
@Temperature 0.000 °C
Melting Point 1064 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.040
@Temperature 100 °C
total spectrum
Reflection Coefficient, Visible (0-1) 0.85600 nm
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 300 °C
 
Component Elements PropertiesOriginal ValueComments
Gold, Au >= 99.95 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gold, Au
Commercial Fine Gold, Cast
Copper, Cu; Annealed
Commercial Fine Gold, 60% Reduction
Gold, Au; 18K, White Composition Spec (UNS P00275)

MPAu01 / 12540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.