MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® NRG 1001 PA 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Extrusion/Tubing Grade

Material Notes: VESTAMID®NRG 1001 is a plasticized PA 12 compound with heat and light stabilizers for the extrusion of flexible tubing and hoses especially for oil and petrochemical applications. VESTAMID®NRG 1001 is characterized by easy processing and good dimensional control during pipe extrusion, especially when processing large pipe diameters. Properties of compounds based on polyamide 12 vary little with changing humidity due to low moisture absorption Parts made of the described semi-crystalline material are characterized by exceptional impact strength, low coefficient of sliding friction and good chemical resistance.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccISO 1183
Viscosity Number 100 cm³/gISO 307
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 46.0 MPaISO 527
Elongation at Break >= 200 %ISO 527
Elongation at Yield 5.0 %ISO 527
Tensile Modulus 1400 MPaISO 527
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 4.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 5.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 178 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 120 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75
Vicat Softening Point 140 °C
@Load 5.10 kg
Method B; ISO 306
 170 °C
@Load 1.02 kg
Method A; ISO 306
 
Descriptive Properties
ColorNatural color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTAMID® NRG 2101 PA 12
Evonik VESTAMID® NRG 6001 PA 12
Evonik VESTAMID® LX9008 PA 12
Evonik VESTAMID® NRG 3001 PA 12
Evonik Vestamid® Terra DD G16 Nylon 1012

PEVONIL267 / 196471

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.