MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik TEGO® Antifoam 2280 Emulsion
Categories: Other Engineering Material

Material Notes: Product description: TEGO® Antifoam 2280 is an organic antifoam emulsion based on polyethers.

Application: TEGO® Antifoam 2280 destroys foam or prevents foam formation reliably in formulations produced with dispersing agents like cellulose or polyvinyl alcohols:

  • Polyvinyl acetat (PVAc)
  • Ethylene-Vinyl-Acetate-Copolymers (EVAc)
  • S-PVC
      Special technical information regarding

      Properties / Benefits: TEGO® Antifoam 2280 might be used in all steps for the production of dispersions like reaction, blow down and stripping and for further formulating of the produced dispersions. TEGO® Antifoam 2280 outperforms conventional organic antifoams in several respects, in particular regarding dispersibility and dilution stability. Furthermore undesirable effects associated with other organic or silicone antifoams can be reduced or even eliminated.

      Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
pH 6.0 - 8.06.0 - 8.0
Viscosity 2000 cP2000 cPdynamic
 
Descriptive Properties
Appearancewhite emulsion
Content50%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik TEGO® Antifoam PVC 100 Organomodified siloxane
BASF Glacial Acrylic Acid
BYK Laponite® JS Clay Additive
Solvay RHODAFAC® RE-610 E Surfactant
Henkel Turco Nova EC-202L Etchant

PEVONIL544 / 196748

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.