MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales
metalmen Is Your Direct to US Manufacturing Source for High Purity Metals

(Viewing data as-entered. Click here to return)
Zinc, Zn
Categories: Metal; Nonferrous Metal; Zinc Alloy; Pure Element

Material Notes: Applications: corrosion protection (galvanization), architectural, automotive, batteries, toys.

This entry is for pure Zn. A wide range of zinc alloys is also included in MatWeb.

Key Words: EN 988 (Min. 99.99%) is a common sheet spec.
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.10 g/cc
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 65.391995
Atomic Number 30
Thermal Neutron Cross Section 1.06 barns/atom
X-ray Absorption Edge 1.283 ÅK
 10.33 ÅLI
 11.8395 ÅLII
 12.1055 ÅLIII
Electrode Potential -0.760 V
Electronegativity 1.65Pauling
Ionic Radius 0.740 ÅCrystal Ionic Radius for Valence +2
 0.880 ÅCrystal Ionic Radius for Valence +1
Electrochemical Equivalent 1.219 g/A/h
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 30
Tensile Strength, Ultimate 37.0 MPacast sample
Modulus of Elasticity 96.5 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000005916 ohm-cm
Magnetic Susceptibility -1.74e-7cgs/g
Critical Magnetic Field Strength, Oersted 53.97 - 54.03
Critical Superconducting Temperature 0.840 - 0.860 K
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 110 J/g
Heat of Vaporization 1754 J/g
CTE, linear 31.2 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.3898 J/g-°C
Thermal Conductivity 112.2 W/m-K
Melting Point 419.58 °C
Boiling Point 907 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.050
@Temperature 300 °C
unoxidized or oxidized
 
Component Elements PropertiesOriginal ValueComments
Zinc, Zn 100 %
 
Descriptive Properties
CAS Number7440-66-6

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum, Al
Titanium, Ti
Silver, Ag
Iron, Fe
Nickel, Ni

AMEZn00 / 132

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.