CALIBRE® 603 is a branched polycarbonate resin and is equipped with a mold release and a UV stabilization package. CALIBRE 603 resins exhibit an excellent property balance of high clarity, high melt strength and impact resistance. The CALIBRE 603 resins have high zero-shear viscosity which allow extrusion of complex sheet structures for the building industry or extrusion blow molding of large products without sagging. Available Melt Flow Rates: 3, 5. Data provided by Dow Chemical. |