MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain Norton® Tygon® R-1000 Ultra-Soft Tubing Formulation  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: Replaced by Tygon® S3 E-1000. Description: Tygon® R-1000: Tygon® Ultra-Soft Tubing resists a broad range of aqueous chemicals and provides an excellent alternative to silicone tubing in applications where corrosive chemicals are used. Its minimal resistance to compression permits use in low-torque pump applications including battery driven types. Tygon® Ultra-Soft Tubing stays flexible at temperatures as low as -100°F (-73°C ). Its smooth bore facilitates easy cleaning and helps prevent possible buildup. Do not autoclave.

Features/Benefits:
  • Ultra-soft and flexible
  • Performs well at low temperatures (to -100°F)
  • Excellent for use in low-torque pump applications
  • Resistant to a broad range of corrosive chemicals
  • Meets FDA 21 CFR Part 177.2600
Typical applications include General Laboratory, Analytical Instruments, Peristaltic Pumps, and Vent and Drain Lines.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792-91
Water Absorption 0.30 %24 hours at 23°C; ASTM D570-95
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 4015 seconds; ASTM D2240-97
Tensile Strength, Yield 1200 psiASTM D412-97
Elongation at Break 375 %ASTM D412-97
100% Modulus 0.330 ksi
@Strain 100 %
ASTM D412-97
Tear Strength 52.0 pliInitial Tear Strength; ASTM D1004-94
Compression Set 57 %
@Temperature 70.0 °C
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
Tensile Set 73 %ASTM D412-97
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 500 V/milASTM D149-95
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °F
Brittleness Temperature -103 °FASTM D746-95
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
ColorClear

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Norton® Tygon® 2075 Ultra Chemical Resistant Tubing Formulation
Saint-Gobain Tygon® 2275 High Purity Tubing Formulation
Saint-Gobain Tygon® Noroprene® Chemical Tubing Formulation
Saint-Gobain Tygon® LP 1500 Low Permeation Fuel Tubing
Saint-Gobain Tygon® A-60-N Drinking Water Tubing Formulation

PSTGQZ197 / 68711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.