MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Beta Titanium Alloy
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Beta Titanium Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.24 - 5.06 g/ccAverage value: 4.81 g/cc Grade Count:106
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 290 - 485Average value: 363 Grade Count:14
Hardness, Knoop 315 - 535Average value: 396 Grade Count:14
Hardness, Rockwell C 30.0 - 50.0Average value: 38.4 Grade Count:17
Hardness, Vickers 240 - 511Average value: 374 Grade Count:31
Tensile Strength, Ultimate 700 - 1730 MPaAverage value: 1190 MPa Grade Count:110
Tensile Strength, Yield 290 - 1520 MPaAverage value: 1070 MPa Grade Count:95
Elongation at Break 0.000 - 29.0 %Average value: 10.8 % Grade Count:106
Reduction of Area 6.00 - 83.2 %Average value: 33.2 % Grade Count:44
Modulus of Elasticity 63.0 - 186 GPaAverage value: 105 GPa Grade Count:105
Compressive Yield Strength 800 - 1370 MPaAverage value: 1100 MPa Grade Count:17
Compressive Modulus 97.2 - 112 GPaAverage value: 109 GPa Grade Count:8
Notched Tensile Strength 580 - 1600 MPaAverage value: 1180 MPa Grade Count:16
Ultimate Bearing Strength 1300 - 2270 MPaAverage value: 1880 MPa Grade Count:12
Bearing Yield Strength 1270 - 1910 MPaAverage value: 1590 MPa Grade Count:12
Poissons Ratio 0.300 - 0.360Average value: 0.326 Grade Count:74
Fatigue Strength 120 - 1140 MPaAverage value: 616 MPa Grade Count:32
Fracture Toughness 31.0 - 160 MPa-m½Average value: 69.6 MPa-m½ Grade Count:31
Shear Modulus 27.0 - 45.9 GPaAverage value: 40.4 GPa Grade Count:74
Shear Strength 538 - 793 MPaAverage value: 690 MPa Grade Count:14
Charpy Impact 8.00 - 30.0 JAverage value: 14.6 J Grade Count:10
Charpy Impact, Notched 25.0 - 59.0 J/cm²Average value: 33.5 J/cm² Grade Count:4
Bend Radius, Minimum 2.00 - 4.50 tAverage value: 3.60 t Grade Count:5
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000135 - 0.000163 ohm-cmAverage value: 0.000148 ohm-cm Grade Count:88
Magnetic Permeability 1.00Average value: 1.00 Grade Count:17
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.06 - 10.4 µm/m-°CAverage value: 8.88 µm/m-°C Grade Count:84
Specific Heat Capacity 0.490 - 0.710 J/g-°CAverage value: 0.520 J/g-°C Grade Count:94
Thermal Conductivity 6.20 - 8.70 W/m-KAverage value: 7.56 W/m-K Grade Count:80
Melting Point 1550 - 1750 °CAverage value: 1610 °C Grade Count:16
Solidus 1550 - 1670 °CAverage value: 1570 °C Grade Count:16
Liquidus 1600 - 1750 °CAverage value: 1660 °C Grade Count:16
Maximum Service Temperature, Air 288 - 816 °CAverage value: 484 °C Grade Count:33
Beta Transus 700 - 1020 °CAverage value: 778 °C Grade Count:98
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.800 - 6.50 %Average value: 3.06 % Grade Count:96
Boron, B 0.0300 %Average value: 0.0300 % Grade Count:20
Carbon, C 0.0200 - 0.100 %Average value: 0.0661 % Grade Count:81
Chromium, Cr 2.00 - 11.0 %Average value: 5.17 % Grade Count:29
Hydrogen, H 0.0125 - 0.0200 %Average value: 0.0156 % Grade Count:80
Iron, Fe 0.120 - 6.00 %Average value: 0.803 % Grade Count:91
Molybdenum, Mo 4.00 - 16.0 %Average value: 11.1 % Grade Count:54
Nickel, Ni 0.0500 %Average value: 0.0500 % Grade Count:7
Niobium, Nb (Columbium, Cb) 2.20 - 30.0 %Average value: 4.39 % Grade Count:17
Nitrogen, N 0.0300 - 0.0800 %Average value: 0.0510 % Grade Count:78
Oxygen, O 0.100 - 0.500 %Average value: 0.158 % Grade Count:86
Silicon, Si 0.0700 - 0.250 %Average value: 0.180 % Grade Count:20
Sulfur, S 0.0100 %Average value: 0.0100 % Grade Count:7
Tin, Sn 2.00 - 7.00 %Average value: 3.37 % Grade Count:42
Titanium, Ti 70.0 - 93.0 %Average value: 78.6 % Grade Count:110
Vanadium, V 5.00 - 16.0 %Average value: 11.1 % Grade Count:64
Yttrium, Y 0.00200 - 0.00500 %Average value: 0.00485 % Grade Count:20
Zirconium, Zr 2.00 - 11.0 %Average value: 5.69 % Grade Count:48

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Alpha/Beta Titanium Alloy
Overview of materials for Alpha/Near Alpha Titanium Alloy
Overview of materials for Stainless Steel
Overview of materials for Unalloyed/Modified Titanium
Titanium Alloys, General

M01072 / 81700

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.