MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® B 50 H1 PA66/6, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66

Material Notes: Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is available in natural, black, and in other colors upon request.

Benefits: This phosphorus and halogen free flame retardant grade, UL94 V0 at 0.4mm, offers excellent filling qualities together with good stiffness.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: Connectivity- junction blocks, terminal blocks, connectors…

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183/A
Water Absorption 1.1 %
@Temperature 23.0 °C,
Time 86400 sec
1.1 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Viscosity  25 cP
@Shear Rate 100 1/s,
Temperature 290 °C
25 cP
@Shear Rate 100 1/s,
Temperature 554 °F
 27 cP
@Shear Rate 1000 1/s,
Temperature 290 °C
27 cP
@Shear Rate 1000 1/s,
Temperature 554 °F
 29 cP
@Shear Rate 1000 1/s,
Temperature 270 °C
29 cP
@Shear Rate 1000 1/s,
Temperature 518 °F
 30 cP
@Shear Rate 1000 1/s,
Temperature 260 °C
30 cP
@Shear Rate 1000 1/s,
Temperature 500 °F
 107 cP
@Shear Rate 100 1/s,
Temperature 270 °C
107 cP
@Shear Rate 100 1/s,
Temperature 518 °F
 109 cP
@Shear Rate 100 1/s,
Temperature 260 °C
109 cP
@Shear Rate 100 1/s,
Temperature 500 °F
 109 cP
@Shear Rate 10 1/s,
Temperature 290 °C
109 cP
@Shear Rate 10 1/s,
Temperature 554 °F
 120 cP
@Shear Rate 10 1/s,
Temperature 270 °C
120 cP
@Shear Rate 10 1/s,
Temperature 518 °F
 130 cP
@Shear Rate 10 1/s,
Temperature 260 °C
130 cP
@Shear Rate 10 1/s,
Temperature 500 °F
Linear Mold Shrinkage 0.011 cm/cm0.011 in/inIsotropy
Linear Mold Shrinkage, Flow 0.011 cm/cm0.011 in/in
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psiISO 527 Type 1A
Tensile Strength, Yield 80.0 MPa11600 psiISO 527 type 1 A
 85.0 MPa12300 psiASTM D638
Tensile Stress at Strain  35.0 MPa
@Strain 1 %
5080 psi
@Strain 1 %
 62.0 MPa
@Strain 2 %
8990 psi
@Strain 2 %
 75.0 MPa
@Strain 3 %
10900 psi
@Strain 3 %
 78.0 MPa
@Strain 4 %
11300 psi
@Strain 4 %
Elongation at Break 10 %10 %ISO 527 Type 1A
 10 %10 %ASTM D638
Elongation at Yield 4.0 %4.0 %ISO 527 type 1 A
Tensile Modulus 3.60 GPa522 ksiISO 527 Type 1A
Flexural Strength 105 MPa15200 psiISO 178
 120 MPa17400 psiASTM D790
Flexural Modulus 3.65 GPa529 ksiISO 178
Izod Impact, Notched 0.600 J/cm1.12 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched 9.00 J/cm²42.8 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.450 J/cm²2.14 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant 3.63.6IEC 60250
Dielectric Strength 34.0 kV/mm864 kV/inIEC 60243
Dissipation Factor 0.0200.020IEC 60250
Comparative Tracking Index 575 V575 VSolution B; IEC 60112
 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 242 °C468 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FISO 75/Af
UL RTI, Electrical 120 °C
@Thickness 0.380 - 3.00 mm
248 °F
@Thickness 0.0150 - 0.118 in
UL RTI, Mechanical with Impact 90.0 °C
@Thickness 0.750 - 3.00 mm
194 °F
@Thickness 0.0295 - 0.118 in
Flammability, UL94  V-0
@Thickness 0.380 mm
V-0
@Thickness 0.0150 in
1210
 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
1210
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
1210
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
1210
Oxygen Index 33 %33 %ISO 4589
Glow Wire Ignition Temperature 650 °C
@Thickness 1.60 mm
1200 °F
@Thickness 0.0630 in
ISO 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
ISO 60695-2-12
 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
ISO 60695-2-12
 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 240 - 250 °C464 - 482 °F
Front Barrel Temperature 250 - 260 °C482 - 500 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone245-255°C
Fire and smoke F indexI2/F3NF F 16 101

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated
Domo TechnylStar™ S 60G1 V30 PA6, 30% glass filled, DRY
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant
Domo TECHNYL® B 50H1 Natural L PA 66/6, Conditioned

PRHOD747 / 137978

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.