MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultraform® N 2640 Z4 BK140 Q600 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: Ultraform N2640 Z4 BK140 Q600 is a high toughness, elastomer-modified injection molding POM grade.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ISO 1183
Water Absorption 0.80 %0.80 %ISO 62
Moisture Absorption at Equilibrium 0.25 %0.25 %23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.019 cm/cm0.019 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 36.0 MPa5220 psi50mm/min; ISO 527
Elongation at Break >= 50 %>= 50 %50mm/min, Nominal strain; ISO 527
Elongation at Yield 14 %14 %50mm/min; ISO 527
Tensile Modulus 1.55 GPa225 ksi1mm/min; ISO 527
Flexural Modulus 1.57 GPa228 ksiASTM Test
 1.74 GPa252 ksiISO Data
Izod Impact, Notched 0.950 J/cm
@Thickness 3.17 mm
1.78 ft-lb/in
@Thickness 0.125 in
ASTM Test
Izod Impact, Notched (ISO) 11.7 kJ/m²5.57 ft-lb/in²ISO Test
 
Thermal PropertiesMetricEnglishComments
Melting Point 167 °C333 °F10 K/min
 167 °C333 °FASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FASTM Test
 
Descriptive Properties
ColorBK140
Commercial StatusActive America
Impact ModifiedYes
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultraform® N 2640 Z4 UNC Q600 POM
BASF Ultraform® N2640 E4 POM
A. Schulman CPP30GF33BK 30% Mineral Filled, Heat-Stabilized, Homopolymer Polypropylene
BASF Ultraform® N 2320 003 UNC Q600 POM
BASF Ultraform® N2320 006 POM

PBASF9107 / 84871

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.