MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay A5000 FEP Fluoropolymer
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP)

Material Notes: Description: Release film. Ideally suited to aerospace applications.

Features & Benefits:

  • High temperature fluoropolymer, which has been an aerospace industry standard product for many years
  • Exhibits excellent elongation and release properties, and is suitable for use with all prepreg systems including polyester, epoxy, phenolic and BMI
  • Effective at overcoming bridging on the most difficult of contoured shapes.
  • Most commonly used in aerospace applications with numerous OEM approvals
  • Imparts a gloss finish to molding surfaces
  • Available with an etched surface on one side to aid bonding to rubber products for use as a localized pressure pad/intensifier
  • Available perforated and non-perforated

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 25.0 - 50.0 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 3500 psi
Elongation at Break 300 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
 
Descriptive Properties
ColorRed, white and violet
Yield18.5 m2/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
Daikin NEOFLON® NP-20 FEP
AGC LUMIFLON® LF-200 Fluoropolymer Resin
AGC LUMIFLON® FE-4400 Isocyanate Comparison Fluoropolymer Resin
Chemours Teflon® PTFE Grade K-10 Fluoropolymer Resin

PCYTED272 / 180574

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.