MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC LUMIFLON® LF-200 Fluoropolymer Resin
Categories: Polymer; Thermoset; Fluoropolymer, TS

Material Notes: LUMIFLON fluoropolymer resins were developed in 1982 as the first solvent-soluble fluoropolymers in the world. LUMIFLON polymers consist of alternating fluoroethylene and alkyl vinyl ether segments (FEVE). The fluorinated segments provide outstanding UV stability, weather resistance, and chemical resistance, while the vinyl ether segments provide solvent compatibility and cross-linking sites. LUMIFLON resins are used to make ultra-weatherable coatings for architectural, aerospace, automotive, and industrial maintenance markets. LUMIFLON LF-200 is a moderate molecular weight, moderate OH number resin. It is typically used in applications where outstanding weathering is required, but only moderate chemical resistance. Markets include architectural coatings, light duty industrial coatings, and coatings for concrete.

Product Characteristics:

  • Moderate OH functionality
  • Excellent weatherability and water resistance, good chemical resistance
  • Excellent adhesion to primers, fiberglass, plastics, and composites
  • Wide range of gloss possible
  • Curable at both ambient and elevated temperatures
  • Suitable for shop and field applied coatings

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/cc
Solids Content 60 %60 %
Viscosity 2240 cP2240 cP
 
Mechanical PropertiesMetricEnglishComments
Impact  >= 0.50
@Diameter 12.7 mm
>= 0.50
@Diameter 0.500 in
[m], Extrusion 0.5 kg; ASTM D2794
 >= 1.5
@Diameter 12.7 mm
>= 1.5
@Diameter 0.500 in
[m], Intrusion 0.5 kg; ASTM D2794
 
Optical PropertiesMetricEnglishComments
Gloss 70 %70 %20°; ISO 2813
 83 %83 %60°; ISO 2813
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 min168 hour23
 
Descriptive Properties
AppearanceClear Liquid
Hardness3HPencil, ASTM D3363
OH Number52[mg KOH/g]-polymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay A5000 FEP Fluoropolymer
Solvay AVIMID® RB Polyimide Composite
Solvay AVIMID® N Polyimide Composite
Saint-Gobain Norton® FEP Fluoropolymer Film
Evonik Rohacell® 110EC-5 Electrically Conductive Grade Polymethacrylimide (PMI) Foam

PAGCX133 / 191242

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.