MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ceradyne Ceralloy® 147-1E Silicon Nitride  (discontinued **)
Categories: Ceramic; Nitride

Material Notes: Ceralloy® 147 Hot Pressed Silicon Nitride (HPSN) can be formulated into a variety of compositions having minimal densification aids. These HPSN compositions offer the highest strength of Ceradynes silicon nitrides. Finished components are machined at Ceradynes precision diamond grinding facility.

Applications: wear components, semi conductor components.

Information provided by Ceradyne Company

Ceradyne was acquired by 3M in 2012. The product line has been extensively renamed and reconfigured.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.10 g/cc
Weibull Modulus 18
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 18000.3 kg/mm²
Modulus of Elasticity 310 GPa
Flexural Strength 700 MPa
@Temperature 23.0 °C
Poissons Ratio 0.27
Fracture Toughness 5.00 MPa-m½
Shear Modulus 122 GPacalculated
Abrasion 1030Abrasive Wear Resistance Parameter
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 ohm-cm
Dielectric Constant 9.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.20 µm/m-°C
@Temperature 20.0 - 1000 °C
Thermal Conductivity 42.0 W/m-K
 
Descriptive Properties
Purity, %>98.5
Thermal Shock Parameter540°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Techical Ceramics Ekasic® S Silicon Nitride
Ceradyne Ceralloy® 147-5 Silicon Nitride
Silicon Nitride
3M Techical Ceramics Ekatherm® Silicon Nitride
Ceradyne Ceralloy® 147-A Hot Pressed Silicon Nitride (Si3N4)

CCERDN04 / 687

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.