MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PolyMirae Moplen EP649N Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Moplen EP649N is a medium flow heterophasic copolymer development grade with outstanding mechanical properties and antistatics. The product features an easy processability and an excellent stiffness combined with good impact properties and high gloss. This grade is suitable for a wide range of appliances parts, Toys and consumer goods industries. Moplen EP649N resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact.

Product Features: High gloss/ Good stiffness and Impact balance /Excellent antistatic property

Typical Applications: Refrigerator/Vacuum Cleaner/Washing Machine parts/Toys/Houseware

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASMT D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 105ASTM D785
Tensile Strength, Yield 320 kg(f)/cm²ASTM D638
Elongation at Yield 7.0 %ASTM D638
Flexural Modulus 18500 kg(f)/cm²ASTM D790
Izod Impact, Notched 4.00 kg-cm/cm
@Temperature -20.0 °C
ASTM D256
 10.0 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °CASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 3429 Polypropylene, Injection Molding Grade
Total PPH 3825 Polypropylene, Injection Molding Grade
Total PPH 3230 Polypropylene, Blow Molding Grade
Telles Mirel™ P1003 Injection Molding Grade PHA Bioplastic
Spartech EP5140 Talc Filled Homopolymer

PMIRAF30 / 183251

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.