MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain Rulon® W2 Bearing/Seal PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are used in bearing and seal applications from temperature extremes of 400°F to over 500°F with and without additional lubricants. A unique property of Rulon® is the absence of stick slip, that is, erratic low-speed motion. PTFE = polytetrafluoroethylene

W2 Grade Bearing/Seal PTFE: Specifically developed for fresh water bearing and seal applications, Rulon W2 has the lowest wear rate in wet environment of any standard Rulon. Black in color. Suitable for wet, dry, or vacuum environments. Mating surface of Rc 25 or higher steel/stainless steel. Material does not have electrical and thermal insulation properties. Markets for W2 grade include Appliances, Automotive, Industrial, Transportation.
Information provided by Saint Gobain Performance Products.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.10 g/ccASTM D792
Water Absorption 0.00 %
@Time 86400 sec
ASTM D570
Deformation 3.0 %
@Pressure 10.3 MPa
24 hrs; ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 64
Hardness, Rockwell B 25
Tensile Strength 12.4 MPaASTM D638
Elongation at Break 70 %ASTM D638
Compressive Yield Strength 5.90 MPa
@Strain 1 %
Mold Direciton; ASTM D695
 6.20 MPa
@Strain 1 %
Cross Direciton; ASTM D695
Coefficient of Friction, Dynamic 0.15 - 0.30
Coefficient of Friction, Static 0.15 - 0.30
Limiting Pressure Velocity 10000 psi-ft/min
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µin/in-°F
@Temperature 25.6 - 93.3 °C
Length
 63.0 µin/in-°F
@Temperature 25.6 - 149 °C
Length
CTE, linear, Transverse to Flow 47.0 µin/in-°F
@Temperature 25.6 - 93.3 °C
Diameter
 49.0 µin/in-°F
@Temperature 25.6 - 149 °C
Diameter
Thermal Conductivity 4.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 288 °C
Minimum Service Temperature, Air -240 °C
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Rulon® XL Bearing/Seal PTFE
Saint-Gobain Rulon® J Bearing/Seal PTFE
Saint-Gobain Rulon® 641 Bearing/Seal PTFE
Saint-Gobain Rulon® 945 Bearing/Seal PTFE
Saint-Gobain Rulon® 1337 Bearing/Seal PTFE

PSTGQZ173 / 68687

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.