MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SYNTHOS Koplen® 0814 F Expandable Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Self-Extinguishing type Koplen®.

Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to moldings and block.

Specific Characteristics: Flammability according to CSN EN ISO 11925-2, class E and DIN 4102-B1. Shorter processing cycle than for type 1020F.

Typica Application: Large-size molded blocks. Molded boards. Cut boards and building insulation profiles acc CSN EN 13163

Synthos was formerly known as Kaucuk. All information provided by Synthos.

Key Words: EPS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.0160 g/ccMinimum
 0.0160 - 0.0400 g/ccTypical
Particle Size 900 - 1250 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
NOVA Chemicals Expandable Polystyrene (EPS) 33MB Expandable Polystyrene Resin
Jackon JACKOCELL® S332 Expanded Polystyrene Packaging and Shape Molding
Ineos Nova T163B Expandable Polystyrene

PSYNT036 / 82649

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.