MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SEKISUI SPI KYDEX® 100 Polymer Alloy Sheet
Categories: Polymer; Thermoplastic

Material Notes: High impact fire-rated sheet

Super tough, durable KYDEX® 100, a proprietary alloy sheet, brings new dimensions to thermoformers in: formability, rigidity, breakage resistance, chemical resistance and fire retardancy.

KYDEX® 100 is available in a wide range of standard and custom colors, textures, and sheet sizes. It is Underwriters Laboratories, Inc® recognized for UL Std 94 V-0, 5V and has 961 J/m (18 ft-lbs/in) Notched Izod impact resistance.

Suggested Applications:

  • Aircraft Interiors
  • Mass Transit Vehicle Interior Components
  • Equipment Housings
  • Medical Products
  • Miscellaneous Applications

Features:

  • Good for deep or hard to form parts more rigid, parts will deform less when loaded
  • High Notched Izod impact resistance offers unsurpassed resistance to breakage
  • Meets highest standard for chemical resistance for thermoplastic materials
  • Recognized by Underwriters Laboratories, Inc® for Std 94 V-0, 5V in all thicknesses and colors
  • Uniform wall thickness and crisp detail
  • Easy machining and fabricating using conventional method for equipment

Values based upon 3.18 mm(0.125 in) sheet unless otherwise specified

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 94ASTM D785
Tensile Strength 42.0 MPaASTM D638
Elongation at Break 160 %ASTM D638
Modulus of Elasticity 2.31 GPaASTM D790
Flexural Strength 63.0 MPaASTM D790
Izod Impact, Notched 961 J/m
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Transverse to Flow 42.0 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 173 °FAnnealed; ASTM D648
Flammability, UL94 V-0UL File E115252; Component Recognition
 5VB
@Thickness >=0.711 mm
Underwriters Laboratories., Inc®, File E115252; Component Recognition; UL Standard 94
 
Descriptive Properties
Flammability0.90 mmDIN 5510-2 (S4, ST2, SR2)
 6.50 mmDIN 5510-2 (S4, ST2, SR1)
 Class 1BS 476 Part 7 (3.20 mm)
 Class 1YBS 476 Part 7 (3.00 mm)
 PassEC 95/28/EG (1.00 - 6.00 mm)
 PassFAR 25.853(a)(ii); Vertical Burn, 12 sec
 PassFAR 25.853(a)(i); Vertical Burn, 60 sec
Motor Vehicle Safety StandardPassMVSS 302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Stratasys® Ultem 9085 for Rapid Prototyping
Magnesium ZK40A-T5, Extruded
Magnesium ZE41A-T5, Cast
SEKISUI SPI KYDEX® T Thermoplastic
SEKISUI SPI KYDEX® 410 ABS/PVC

PSEKIS030 / 185855

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.