MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Durethan® BKV 30 FN00 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: PA6, injection molding grade, 30% glass fibers, UL94 V-0 at 0,75 mm , free of halogen and red phosphorus, glow wire flammability test max. 960°C

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.427 g/ccISO 1183
Moisture Absorption at Equilibrium 1.5 %50% RH; ISO 62
Water Absorption at Saturation 5.0 %IOS 62
Linear Mold Shrinkage, Flow 0.0022 cm/cm60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0062 cm/cm60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Melt Flow 23 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 90.0 MPa5 mm/min; ISO 527-1,-2
Elongation at Break 6.1 %5 mm/min; ISO 527-1,-2
Tensile Modulus 6700 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 140 MPa2 mm/min; ISO 178-A
Flexural Yield Strength 128 MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 6000 MPa2 mm/min; ISO 178-A
Flexural Strain at Break 4.6 %2 mm/min; ISO 178-A
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1U
Charpy Impact Unnotched 65.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
 
Thermal PropertiesOriginal ValueComments
Melting Point 224 °C10°C/min (Dry); ISO 11357-1,-3
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °Cinjection molding
 250 - 270 °C
Mold Temperature 80.0 °Cinjection molding
 80.0 - 100 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 30 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 H2.0 EF DUS029 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 G H2.0 900051 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 25 FN01 000000 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 240 H2.0 XCP 901510 Nylon 6 (PA6), 40% Glass Fiber Reinforced, Dry

PLANW9379 / 208202

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.