MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Surlyn® E185SB Ionomer Resin
Categories: Polymer; Film; Thermoplastic; Ionomer; Ionomer, Film Grade

Material Notes: Surlyn® E185SB is an ionomer of an acid copolymer resin. It is designed for coextrusion with high-density polyethylene in peelable seals applications. It can be used in extrusion equipment designed to typically process polyethylene resins.

Uses:

  • Film
  • Packaging
  • Sealants

Composition: Proprietary Formulation

Surlyn® E185SB can be coextruded with HDPE to provide delamination-type peelable seals. The seal strength can be controlled by processing conditions and/or the thickness of Surlyn® E185SB layer. Thickness is typically in the range of 5 to 15 microns (0.20 to 0.60 mils). Other benefits of Surlyn® E185SB include:

  • Very low seal initiation temperature·
  • Broad sealing temperature range
  • Contains "Slip" and "Antiblock"

Surlyn® E185SB complies with the Food and Drug Administration regulation 21 CFR 175.300 - - ‘Resinous and polymeric coatings’. This regulation describes polymers that may be used as coatings on a metal substrate for packaging, transporting, or holding food, subject to meeting the extractive limitations in the regulation. SURLYN E185SB also complies with FDA regulation 21 CFR 175.320 - - ‘Resinous and polymeric coatings for polyolefin films’, subject to meeting the extractive limitations in the regulation. SURLYN E185SB contains 0.45 wt.% of a slip agent that complies with 21 CFR 175.300(b)(3)(xxv) – ‘Release agents’ and 21 CFR 175.320(b)(3). This slip agent cannot exceed 0.0085 milligram per square centimeter (0.055 milligram per square inch) in the finished food-contact article.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D792, ISO 1183
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
 
Thermal PropertiesMetricEnglishComments
Melting Point 62.0 °C144 °FFreezing Point; ASTM D3418, ISO 3146
 89.0 °C192 °FASTM D3418, ISO 3146
Vicat Softening Point 60.0 °C140 °FASTM D1525, ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 260 °C<= 500 °F
Feed Temperature 135 °C275 °FBlown Film Coextrusion
 135 °C275 °FCast Film/Sheet Processing
Zone 2 160 °C320 °FBlown Film Coextrusion
 160 °C320 °FCast Film/Sheet Processing
Zone 3 185 °C365 °FBlown Film Coextrusion
 185 °C365 °FCast Film/Sheet Processing
Zone 4 185 °C365 °FBlown Film Coextrusion
 210 °C410 °FCast Film/Sheet Processing
Zone 5 185 °C365 °FBlown Film Coextrusion
 210 °C410 °FCast Film/Sheet Processing
Adapter Temperature 185 °C365 °FBlown Film Coextrusion
 210 °C410 °FCast Film/Sheet Processing
Die Temperature 185 °C365 °FBlown Film Coextrusion
 210 °C410 °FCast Film/Sheet Processing
Melt Temperature 160 - 235 °C320 - 455 °FBlown/Cast Film Processing
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Surlyn® 1707 Sodium Ionomer
Dow Surlyn® 6320 Magnesium Ionomer
Dow Surlyn® 7930 Ionomer Resin, Lithium
Dow Surlyn® 9320 Zinc Ionomer
Dow Surlyn® 2601B Sodium Ionomer

PDTA4975 / 170415

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.