MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Paxon™ AM55-003 Blow Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: AM55-003 is a blow molding grade high density polyethylene copolymer containing an excellent antistat additive. It provides a good combination of stiffness and stress crack resistance. AM55-003 contains an antistat which may be used in contact with limited types of food.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.954 g/ccASTM D4883
ESCR 100% Igepal® 25 hourASTM D1693 Condition B
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2100 psiASTM D638
Tensile Strength, Yield 4000 psiASTM D638
Elongation at Break 560 %ASTM D638
Elongation at Yield 8.0 %ASTM D638
Tensile Modulus 290000 psiASTM D638
Flexural Modulus 190000 psiMethod1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790
Tensile Impact Strength 90.0 ft-lb/in²ASTM D1822
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °CASTM D648
Vicat Softening Point 260 °FASTM D1525
Brittleness Temperature <= -105 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Melt Temperature 375 °F
 
Descriptive Properties
FeaturesAntistat and Thermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Paxon™ AU55-003 Blow Molding Resin
ExxonMobil Paxon™ AG45-004 Blow Molding Resin
ExxonMobil HD 5403.AS Blow Molding Resin
ExxonMobil HD 5403 Blow Molding Resin
ExxonMobil HD 5003.AS Blow Molding Resin

PEXB099 / 37404

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.