MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond Supreme 11HT High Temperature Resistant Two Component Epoxy System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Excellent toughness
  • Convenient handling
  • High bond strength in shear and peel modes
  • Thermal stability up to +400°F
  • Withstands thermal cycling
  • Superb adhesion to many substrates
Product Description: Master Bond Supreme 11HT is a high performance, higher viscosity, two part epoxy for bonding and sealing. It is exceptionally easy to use with a one to one mix ratio by weight or volume. Supreme 11HT is a faster setting system and cures readily at room temperature or more quickly at elevated temperatures. The optimum curing schedule is overnight at room temperature, followed by 1 hour at 150-200°F. Supreme 11HT is formulated to have very good toughness, which imparts high bond strengths in both the shear and peel mode. It also allows the system to withstand rigorous thermal cycling as well as impact and shock. Supreme 11HT bonds well to a wide variety of substrates, including metals, glass, ceramics, composites, many rubbers and plastics. It has fine chemical resistance to water, oil and fuels. Upon curing, it is a highly reliable electrical insulator. Most noteworthy is its very wide temperature range of -100°F to +400°F. Additionally, Supreme 11HT has low shrinkage upon curing, dependable dimensional stability and is readily machinable. The color of Part A is gray and Part B is amber. The very user friendly processing and top notch performance profile enables Supreme 11HT to be used in a wide variety of high-tech applications, especially in aerospace, electronics, specialty OEM and related industries.

Product Advantages:

  • Convenient mixing; non-critical one to one mix ratio by weight or volume
  • Easy to apply, higher viscosity system; good flow, fast setting at room temperature
  • Superb adhesion to many different substrates
  • High caliber resistance to severe thermal cycling, impact and shock
  • Stellar dimensional stability
  • Exceptionally robust tensile lap shear strength

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 60000 - 110000 cPPart B, thixotropic
 90000 - 120000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50 - 55
Tensile Strength >= 7600 psi
Adhesive Bond Strength >= 3200 psiTensile Lap, Aluminum to Aluminum
Peel Strength >= 20.0 plialuminum to aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cm
Dielectric Constant 4.7
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 2.00 hour
@Temperature 93.3 °C
 24.0 - 36.0 hour
@Temperature 23.9 °C
Working Life 20.0 - 25.0 minAfter mixing, 100 gram batch
Shelf Life 6.00 - 12.0 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
Cure Scheduleovernight at 75°Fplus 1 hour at 150-200°F
Mixing Ratio1:1 by weightPart A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond Supreme 33 High Temperature Resistant, Structural Adhesive
Master Bond Supreme 11HT-LO Adhesive and Sealant Serviceable to +400°F
Henkel Loctite® Ultra Grey® 5999 Flange Sealant
Henkel Loctite® Ultra Grey® 5699 Flange Sealant
Master Bond Supreme 10AOHT Thermally Conductive One Component Epoxy System

PMASTM958 / 185551

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.