MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bamberger Polymers Bapolene® 345F Medium Density Polyethylene, Film Extrusion Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: This resin is a medium molecular weight film resin with excellent tensile, impact, and tear properties. This product meets US FDA 21 CFR 177.1520.

Applications: Bags; Film

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers.

Key Words: Good Impact Resistance; Good Tear Strength; Good Toughness; High Rigidity; Medium Molecular Weight
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.936 g/ccASTM D-1505
Thickness 25.40 microns
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 300 %2.0 in/min; ASTM D-882
Film Elongation at Break, TD 800 %2.0 in/min; ASTM D-882
Elmendorf Tear Strength MD 15 gASTM D1922
Elmendorf Tear Strength TD 1500 gASTM D1922
Dart Drop Test 50.0 g
@Thickness 0.0254 mm
ASTM D1709A
Film Tensile Strength at Break, MD 51.7 MPa2.0 in/min; ASTM D-882
Film Tensile Strength at Break, TD 37.6 MPa2.0 in/min; ASTM D-882
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
processFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Extruded
Bamberger Polymers Bapolene® 0760 High Density Polyethylene, Blow Molding Grade
Bamberger Polymers Bapolene® 350F High Density Polyethylene, Film Extrusion Grade
Toyobo Dyneema® SK60 High Strength Polyethylene Fiber
Aluminum, Al

PBP3B073 / 20795

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.