MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Orgalloy® RS 6010 NAT Polyamide 6 Alloy 10% Glass Fiber reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled

Material Notes: Polyamide Alloy, Rigid grade, Nylon 6 based
Molding of Engineering Parts

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccISO 1183
 1.12 g/ccCond.; ISO 1183
Water Absorption 3.0 %Dry; Sim. to ISO 62
Moisture Absorption 1.20 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cmDry; ISO 294-4, 2577
 0.0060 cm/cm
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 235 °C
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 76
@Time 15.0 sec
Dry; ISO 7619-1
Tensile Strength, Yield 73.0 MPaCond.; ISO 527-1/-2
 80.0 MPaDry; ISO 527-1/-2
Elongation at Break 4.0 %Dry; ISO 527-1/-2
 4.0 %Cond.; ISO 527-1/-2
Elongation at Yield 3.0 %Dry; ISO 527-1/-2
 3.0 %Cond.; ISO 527-1/-2
Tensile Modulus 3800 MPaCond.; ISO 527-1/-2
 4150 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Cond.; ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
Cond.; ISO 179/1eA
Tensile Creep Modulus, 1 hour 2530 MPaCond.; ISO 899-1
Tensile Creep Modulus, 1000 hours 1790 MPaCond.; ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohmCond.; IEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
Cond; IEC 60250
 3.0
@Frequency 100 Hz
Cond.; IEC 60250
Dielectric Strength 36.0 kV/mmDry; IEC 60243-1
 36.0 kV/mmCond.; IEC 60243-1
Dissipation Factor 0.024
@Frequency 1e+6 Hz
Cond.; 0
 0.063
@Frequency 100 Hz
Cond.; IEC 60250
Comparative Tracking Index 600 VCond.; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 210 °CDry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 190 °CDry; ISO 75-1/-2
Vicat Softening Point 170 °C50°C/h 50N; Dry; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
 HB
@Thickness 3.20 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °CInjection Molding; ISO 294
Mold Temperature 60.0 °CInjection Molding; ISO 10724
 
Descriptive Properties
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
Processing MethodsInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 10% Glass Fiber Filled
Arkema Orgalloy® RS 6630 BLACK Polyamide 6.6 Alloy 30% Glass Fiber reinforced
Arkema Rilsamid® AZM 30 BLACK T6LD PA12-GF30
Covestro Apec® HT KU 1-9357/2 High-Heat Polycarbonate, 20% Glass Fiber
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled

PARKG449 / 24507

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.