MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

DuPont Mobility and Materials Vespel® SP-1 Polyimide, Machined
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Unfilled

Material Notes: Provides maximum physical properties and best electrical and thermal insulation.

Applications: Mechanical and electrical parts at elevated temperatures. Valve seats, seal, insulators.

Direct-formed properties were measured perpendicular to the forming direction unless specified. Machined properties are non-directional

Information provided by DuPont

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.43 g/cc1.43 g/ccASTM D792
Water Absorption 0.24 %0.24 %24 hrs @ 73°F.; ASTM D570
 0.72 %0.72 %48 hrs @ 122°F; ASTM D570
Moisture Absorption at Equilibrium 1.0 - 1.3 %1.0 - 1.3 %50% RH
Deformation 0.14 %0.14 %2000 psi; 122°F; ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 45 - 6045 - 60ASTM D785
Tensile Strength, Ultimate 86.2 MPa12500 psi73°F; ASTM D1708
 41.4 MPa
@Temperature 260 °C
6000 psi
@Temperature 500 °F
ASTM D1708
Elongation at Break 7.5 %7.5 %73°F; ASTM D1708
 6.0 %
@Temperature 260 °C
6.0 %
@Temperature 500 °F
ASTM D1708
Flexural Strength 62.1 MPa9000 psi500°F; ASTM D790
 110 MPa16000 psi73°F; ASTM D790
Flexural Modulus 1.72 GPa250 ksi500°F; ASTM D790
 3.10 GPa450 ksi73°F; ASTM D790
Compressive Strength 24.8 MPa3600 psi@1% strain; 73°F; ASTM D695
 51.0 MPa7400 psi@0.1% Offset; 73°F; ASTM D695
 133 MPa19300 psi@10% strain; 73°F; ASTM D695
Compressive Modulus 2.41 GPa350 ksi73°F; ASTM D695
Poissons Ratio 0.410.4173°F
Fatigue Strength  16.5 MPa
@# of Cycles 1.00e+7 ,
Temperature 260 °C
2400 psi
@# of Cycles 1.00e+7 ,
Temperature 500 °F
Axial Fatigue Endurance Limit
 26.2 MPa
@# of Cycles 1000 ,
Temperature 260 °C
3800 psi
@# of Cycles 1000 ,
Temperature 500 °F
Axial Fatigue Endurance Limit
 42.1 MPa
@# of Cycles 1.00e+7 ,
Temperature 22.8 °C
6100 psi
@# of Cycles 1.00e+7 ,
Temperature 73.0 °F
Axial Fatigue Endurance Limit
 44.8 MPa
@# of Cycles 1.00e+8 ,
Temperature 22.8 °C
6500 psi
@# of Cycles 1.00e+8 ,
Temperature 73.0 °F
Flexural Fatigue Endurance Limit
 55.8 MPa
@# of Cycles 1000 ,
Temperature 22.8 °C
8100 psi
@# of Cycles 1000 ,
Temperature 73.0 °F
Axial Fatigue Endurance Limit
 65.5 MPa
@# of Cycles 10000 ,
Temperature 22.8 °C
9500 psi
@# of Cycles 10000 ,
Temperature 73.0 °F
Flexural Fatigue Endurance Limit
Shear Strength 89.6 MPa13000 psiASTM D732
Izod Impact, Notched 0.427 J/cm0.800 ft-lb/in73°F; ASTM D256
Izod Impact, Unnotched 7.47 J/cm14.0 ft-lb/in73°F; ASTM D256
Coefficient of Friction, Dynamic 0.290.29PV-25,000. Steady State; Unlubricated in air.
Coefficient of Friction, Static 0.350.35In air.
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 - 1.00e+17 ohm-cm1.00e+16 - 1.00e+17 ohm-cm73°F; ASTM D257
Surface Resistance 1.00e+15 - 1.00e+16 ohm1.00e+15 - 1.00e+16 ohm73°F; ASTM D257
Dielectric Constant  3.55
@Frequency 1e+6 Hz
3.55
@Frequency 1e+6 Hz
ASTM D150
 3.62
@Frequency 100 Hz
3.62
@Frequency 100 Hz
ASTM D150
 3.64
@Frequency 10000 Hz
3.64
@Frequency 10000 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm560 kV/inShort time; 80 mils thick; 73°F; ASTM D149
Dissipation Factor  0.0018
@Frequency 100 Hz
0.0018
@Frequency 100 Hz
ASTM D150
 0.0034
@Frequency 1e+6 Hz
0.0034
@Frequency 1e+6 Hz
ASTM D150
 0.0036
@Frequency 10000 Hz
0.0036
@Frequency 10000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  45.0 µm/m-°C
@Temperature -62.2 - 22.8 °C
25.0 µin/in-°F
@Temperature -80.0 - 73.0 °F
ASTM E-228
 54.0 µm/m-°C
@Temperature 22.8 - 300 °C
30.0 µin/in-°F
@Temperature 73.0 - 572 °F
ASTM E-228
Specific Heat Capacity 1.13 J/g-°C0.270 BTU/lb-°F
Thermal Conductivity 0.346 W/m-K2.40 BTU-in/hr-ft²-°F104°F
Deflection Temperature at 1.8 MPa (264 psi) 360 °C680 °FApproximate; ASTM D648
Oxygen Index 53 %53 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® SP-1 ISO Polyimide
DuPont Mobility and Materials Vespel® SP-1 Polyimide, Direct formed
Manifattura Cattaneo VESPEL® SP1 Polyimide
DuPont Mobility and Materials VESPEL TP-8054 Polyimide
Mitsubishi Chemical Advanced Materials Semitron™ MDS 100 PEEK

PDU2000 / 32861

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.