MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Escorene® UL 8705E Adhesive Application Resin
Categories: Polymer; Adhesive; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: Escorene Ultra UL 8705 is a relatively low viscosity, 29% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has good compatibility with both hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt adhesives, glue sticks, sealants and wax blends. UL 8705E contains an additive package to improve pellet flowability and handling.

Availability: Asia Pacific, Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Adhesives and Sealants
  • Glue Sticks
  • Industrial Sealants
  • Low Viscosity Adhesives
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.953 g/ccExxonMobil Method
Viscosity 9300 cP
@Temperature 190 °C
ASTM D3236
Vinyl Acetate Content 27.6 %ExxonMobil Method
Melt Flow 800 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 6915s; ASTM D2240
Hardness, Shore D 1815s; ASTM D2240
Tensile Strength at Break 280 psiASTM D638
Elongation at Break 360 %ASTM D638
Flexural Modulus, 1% Secant 2890 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 °FPeak Melting Temperature; ExxonMobil Method
 
Descriptive Properties
FeaturesThermal Stabilizer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Escorene® UL 8705 Adhesive Application Resin
Arkema EVATANE® 28-800 Copolymer Ethylene - Vinyl Acetate
Honeywell A-C® 400A EVA copolymer
Honeywell A-C® 405T EVA copolymer
ExxonMobil Escorene® UL 7765 Adhesive Application Resin

PEXB167 / 37472

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.