MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Elastollan® 1180A10 Wire & Cable Grade Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: As with all TPU products this grade must be dried prior to processing.

Information provided by BASF Corporation.

Key Words: TPU Rubbers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/cc
@Thickness 2.00 mm
molded plaque, cured 20 hr at 100°C; ASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
@Thickness 2.00 mm
molded plaque, cured 20 hr at 100°C; ASTM D2240
Tensile Strength, Ultimate 48.0 MPa
@Thickness 2.00 mm
molded plaque, cured 20 hr at 100°C; ASTM D412
Tensile Stress at Strain 4.80 MPa
@Strain 100 %
ASTM D-412
 12.0 MPa
@Strain 300 %,
Thickness 0.760 mm
extruded sheet; ASTM D412
Elongation at Break 625 %on 0.030 in extruded sheet; ASTM D-412
Flexural Modulus 0.0300 GPa
@Thickness 2.00 mm
molded plaque, cured 20 hr at 100°C; ASTM D790
Tear Strength 42.0 kN/m
@Thickness 0.760 mm
Split tear strength; extruded sheet; ASTM D1938
Graves Tear Strength 77.0 kN/m
@Thickness 0.760 mm
on extruded sheet; ASTM D624
Taber Abrasion, mg/1000 Cycles 20
@Thickness 2.00 mm
H-18 wheel; molded plaque, cured 20 hr at 100°C.; ASTM D1044
Compression Set 45 %
@Temperature 70.0 °C
22 hr @ 70°C; ASTM D-395; 0.080 in molded plaque after curing 20 hrs at 100°C.
 25 %
@Thickness 2.00 mm
22 hr at 23°C; molded plaque, cured 20 hr at 100°C.; ASTM D395
Tensile Set 32 %at 200% elongation per ASTM D-412 is on 0.030 in extruded sheet.
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 90.0 °C
@Thickness 2.00 mm
molded plaque, cured 20 hr at 100°C; ASTM D1525
Glass Transition Temp, Tg -43.0 °CPellet sample
Flammability, UL94 HB
@Thickness 0.830 mm
Color: NC.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Elastollan® 1175A10W Wire & Cable Grade Polyurethane Elastomer
BASF Elastollan® 1190A10 Wire & Cable Grade Polyurethane Elastomer
BASF Elastollan® 1180A Polyether Type Polyurethane Elastomer
BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer
BASF Elastollan® 1174D Polyether Type Polyurethane Elastomer

PSF988 / 67204

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.