MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gallium, Ga
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 5.445 g/cc
@Temperature 1100 °C
Liquid
 5.492 g/cc
@Temperature 1010 °C
Liquid
 5.72 g/cc
@Temperature 600 °C
Liquid
 5.779 g/cc
@Temperature 500 °C
Liquid
 5.9037 g/cc
@Temperature 29.65 °C
Solid
 5.907 g/cc
@Temperature 20.0 °C
Solid
 5.972 g/cc
@Temperature 200 °C
Liquid
 6.093 g/cc
@Temperature 32.4 °C
Liquid
 6.0947 g/cc
@Temperature 29.8 °C
Liquid
Vapor Pressure 6.281e-9 bar
@Temperature 727 °C
 0.000001279 bar
@Temperature 927 °C
 0.00005636 bar
@Temperature 1127 °C
 0.0009572 bar
@Temperature 1327 °C
 0.00859 bar
@Temperature 1527 °C
 0.04932 bar
@Temperature 1727 °C
 0.205 bar
@Temperature 1927 °C
 1.00 bar
@Temperature 2204 °C
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 69.7231995
Atomic Number 31
Thermal Neutron Cross Section 2.8 barns/atom
X-ray Absorption Edge 1.195 ÅK
 9.535 ÅLI
 10.613 ÅLII
 10.8546 ÅLIII
Electrode Potential -0.520 V
Electronegativity 1.81Pauling
Ionic Radius 0.620 ÅCrystal Ionic Radius for Valence +3
 0.810 ÅCrystal Ionic Radius for Valence +1
Electrochemical Equivalent 2.45 g/A/h
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 50
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000175 ohm-cma-axis
Magnetic Susceptibility -3.10e-7cgs/g
Critical Magnetic Field Strength, Oersted 560Beta
 815Delta
 950Gamma
Critical Superconducting Temperature 5.90 - 6.20 K5.9, 6.2 for Beta Ga
 7.00 KGamma Ga
 7.85 KDelta Ga
 6.28 K
@Pressure >=3500 MPa
Ga II
 7.50 K
@Pressure >=3500 MPa
Ga II′
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 80.4 J/g
Heat of Vaporization 3894 J/g
CTE, linear 58.0 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.330 J/g-°C
Thermal Conductivity 41.0 W/m-K
Melting Point 29.78 °C
Boiling Point 2204 °C
 
Optical PropertiesOriginal ValueComments
Reflection Coefficient, Visible (0-1) 0.713
@Wavelength 589 nm
 0.756
@Wavelength 436 nm
 0.89
@Wavelength 436 nm
Liquid
 0.89
@Wavelength 589 nm
Liquid
 
Component Elements PropertiesOriginal ValueComments
Gallium, Ga 100 %
 
Descriptive Properties
CAS Number7440-55-3

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Indium, In
Gold, Au
Silver, Ag
Aluminum, Al
Chromium, Cr; Recrystallized

AMEGa00 / 38

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.