MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polycasa Vision CAST PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Cast

Material Notes: QUINN CAST vision is produced using QUINN CAST acrylic, which is well known for its high quality and optical excellence. QUINN CAST vision is produced using the same technology as regular CAST sheets, but with special finishing methods to provide the characteristics that make it suitable for use in projection applications. The entire QUINN CAST acrylic range of products offers ease of fabrication and installation, and a stable, lightweight alternative to traditional glass.

QUINN CAST vision is available in three variants to provide the best choice to suit viewing requirements.

  • Vision front: used for front projection, the most commonly used method, where the projector throws images forward on to a screen for an audience to view. The audience must sit between the screen and projector.
  • Vision rear*: when using this sheet, the projector is hidden behind the screen, so no interruptions to the image can occur and projector noise is minimized. This technique is becoming increasingly popular for use at exhibitions and events with a larger audience.
  • Vision through*: this special product is an almost transparent sheet that allows the projection of images but also permits a clear view through the sheet in zones where no image is projected. This screen has a very low contrast and it would be the right choice in areas with low ambient light.

Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polycasa AKRYLON XT PMMA
Zeon Specialty Materials ZEONOR® 750R Cyclo Olefin Polymer
Spartech Polycast SP 1.25 Cell Cast Acrylic
Samyang Trimma® FT6120 I[R] PMMA, Transparent
Polycasa Acryl® G 66 Acrylic, Injection Molding Grade

PSF023H / 66598

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.