MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bohler-Uddeholm AISI A2 Cold Work Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel; Cold Work Steel

Material Notes: Description: AISI A2 is an air- or oil hardening chromiummolybdenum-vanadium alloyed tool steel characterized by

AISI A2 is characterized by:

  • Good machinability
  • High stability after hardening
  • High compressive strength
  • Good hardenability
  • Good wear resistance

Applications: AISI A2 takes a place in the Uddeholm tool steel range between AISI O1 and AISI D2, offering an excellent combination of good wear resistance and toughness. It may be regarded, therefore, as a “universal” cold work steel. For cutting operations the good toughness of AISI A2 gives excellent resistance to chipping of the cutting edge. In many cases tools made from this steel have given better tooling economy than high-carbon, high-chromium steels of the D3/W.-Nr. 2080 type. AISI A2 has much better machining and grinding properties.

Key Words: AISI A2; W.-Nr. 1.2363
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.279 lb/in³hardened to 62 HRC
 0.275 lb/in³
@Temperature 399 °C
hardened to 62 HRC
 0.277 lb/in³
@Temperature 191 °C
hardened to 62 HRC
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 215Soft annealed
Modulus of Elasticity 27500 ksi(hardened to 62 HRC)
 24600 ksi
@Temperature 399 °C
hardened to 62 HRC
 26900 ksi
@Temperature 191 °C
hardened to 62 HRC
Compressive Yield Strength 1350 MPa0.2%, hardened to 50 HRC
 1800 MPa0.2%, hardened to 55 HRC
 2150 MPa0.2%, hardened to 60 HRC
 2200 MPa0.2%, hardened to 62 HRC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.50 µm/m-°C
@Temperature 20.0 - 200 °C
hardened to 62 HRC
Specific Heat Capacity 0.110 BTU/lb-°F
@Temperature 20.0 °C
hardened to 62 HRC
Thermal Conductivity 26.0 W/m-K
@Temperature 20.0 °C
hardened to 62 HRC
 27.0 W/m-K
@Temperature 191 °C
hardened to 62 HRC
 28.5 W/m-K
@Temperature 399 °C
hardened to 62 HRC
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.0 %
Chromium, Cr 5.3 %
Iron, Fe 91.5 %As Balance
Manganese, Mn 0.60 %
Molybdenum, Mo 1.1 %
Silicon, Si 0.30 %
Vanadium, V 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type A2 Tool Steel
Carpenter No. 484® (Carpenter Air-Hard; AISI A2)
Crucible Steel AIRKOOL® (AISI A2) Tool Steel
Bohler-Uddeholm AISI D2 Cold Work Tool Steel
Latrobe LSS™ A2 Tool Steel (ASTM A2)

NBUCOR20 / 15489

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.