MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total 7253X Polypropylene, Random Copolymer Extrusion Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Random copolymer extrusion grade

Stability - Fina 7253X features both superior color and melt flow stability for trouble-free processing.

FDA - Fina 7253X complies with all applicable FDA regulations and may be used under these provisions for food contact and packaging.

Recommended Applications - Fina 7253X is an ideal resin for use in both single and multilayer extrusion applications.

Processing - Fina 7253X resin processes with typical melt temperatures of 370-450°F (199-232°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Permeability 9.40 g mil/ (m2 day)
@Temperature 37.8 °C
90% RH; ASTM E96
Density 0.900 g/ccASTM D1505
Oxygen Transmission 95.0 cc-mm/m²-24hr-atm
@Temperature 23.0 °C
cc-mm/m²-24hr-atm; ASTM D1434
Melt Flow 1.5 g/10 minASTM D1238L
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 23.4 MPaASTM D638
Elongation at Break 11 %ASTM D638
Modulus of Elasticity 0.827 GPaASTM D638
Flexural Modulus 0.689 GPaASTM D790
Izod Impact, Notched 0.694 J/cmASTM D256A
 
Thermal PropertiesOriginal ValueComments
Melting Point 143 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 199 - 232 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Extrusion Grade
Formosa Plastics Formolene® 7307A Copolymer Polypropylene
Formosa Plastics Formolene® 3335E Random Copolymer Polypropylene
Braskem H 604 Thermoforming & Extrusion Polypropylene Homopolymer
Total 3289MZ Polypropylene, Homopolymer Sheet Extrusion and Thermoforming Grade

PFIN89 / 38419

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.