MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Kaolite 3300 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Crystalline Silica. Cast installation. Kaolite 3300 is a high strength bubble alumina, lightweight castable with a high-purity binder. Kaolite 3300 is recommended for transfer lines to secondary ammonia reformers, and other applications where resistance to hydrogen atmospheres and silica pickup is critical.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.505 - 1.682 g/cc
@Temperature 816 °C
0.05437 - 0.06077 lb/in³
@Temperature 1500 °F
fired
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00207 - 0.00345 GPa0.300 - 0.500 ksifired 5 hours at 816°C
 0.00276 - 0.00552 GPa0.400 - 0.801 ksidried 24 hours at 104°C
 0.00620 - 0.01172 GPa0.899 - 1.700 ksifired 5 hours at temp use limit, °C
Compressive Strength  10.3 - 20.7 MPa
@Temperature 816 °C,
Time 18000 sec
1490 - 3000 psi
@Temperature 1500 °F,
Time 5.00 hour
Cold Crushing Strength, fired; ASTM C 133
 13.8 - 24.1 MPa
@Temperature 104 °C,
Time 86400 sec
2000 - 3500 psi
@Temperature 219 °F,
Time 24.0 hour
Cold Crushing Strength, dried; ASTM C 133
 17.2 - 27.6 MPa
@Temperature 1816 °C,
Time 18000 sec
2490 - 4000 psi
@Temperature 3301 °F,
Time 5.00 hour
Cold Crushing Strength, fired; ASTM C 133
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  1.07 W/m-K
@Temperature 815 °C
7.43 BTU-in/hr-ft²-°F
@Temperature 1500 °F
ASTM C201
 1.08 W/m-K
@Temperature 1093 °C
7.50 BTU-in/hr-ft²-°F
@Temperature 1999 °F
ASTM C201
 1.15 W/m-K
@Temperature 1371 °C
7.98 BTU-in/hr-ft²-°F
@Temperature 2500 °F
ASTM C201
 1.18 W/m-K
@Temperature 538 °C
8.19 BTU-in/hr-ft²-°F
@Temperature 1000 °F
ASTM C201
 1.43 W/m-K
@Temperature 260 °C
9.92 BTU-in/hr-ft²-°F
@Temperature 500 °F
ASTM C201
Maximum Service Temperature, Air <= 1816 °C<= 3301 °F
Shrinkage  0.00 - 0.20 %
@Treatment Temp. 104 °C,
Time 86400 sec
0.00 - 0.20 %
@Treatment Temp. 219 °F,
Time 24.0 hour
dried; ASTM C113
 0.10 - 0.30 %
@Treatment Temp. 816 °C,
Time 18000 sec
0.10 - 0.30 %
@Treatment Temp. 1500 °F,
Time 5.00 hour
fired; ASTM C113
 0.00 - 0.60 %
@Treatment Temp. 1816 °C,
Time 18000 sec
0.00 - 0.60 %
@Treatment Temp. 3301 °F,
Time 5.00 hour
fired; ASTM C113
 
Processing PropertiesMetricEnglishComments
Moisture Content 11 - 13 %11 - 13 %casting by vibrating
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Al2O3 94 %94 %
CaO 4.6 %4.6 %
Fe2O3 0.10 %0.10 %
K2O+Na2O 0.40 %0.40 %Na2O & K2O
MgO 0.10 %0.10 %
SiO2 0.50 %0.50 %
 
Descriptive Properties
Placement, average (kg)44

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Thermal Ceramics Kaocast 3000 Dense Castable
Thermal Ceramics Kaolite 3300 High Temperature Insulating Castables
Thermal Ceramics Kaocrete HPM 90 Ultra High Strength Castables
Morgan Advanced Ceramics Kao-Tab® Monolithics 95 Thermal Ceramic
Morgan Advanced Ceramics Alumor 90 Thermal Ceramic

CMORF6272 / 203056

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.