MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Delrin Delrin® 300TE BK602 POM-I
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Toughened Medium-high Viscosity Acetal Homopolymer with Very Low Emissions

Information provided by DuPont; Delrin was sold by DuPont in 2023.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183
Melt Density 1.15 g/cc
@Temperature 205 °C
0.0415 lb/in³
@Temperature 401 °F
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.015 cm/cm0.015 in/inISO 294-4, 2577
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 6969ISO 2039-2
Hardness, Rockwell R 116116ISO 2039-2
Tensile Strength, Yield 54.0 MPa7830 psiISO 527-1/-2
Elongation at Break 35 %35 %Nominal; ISO 527-1/-2
Elongation at Yield 20 %20 %ISO 527-1/-2
Tensile Modulus 2.00 GPa290 ksiISO 527-1/-2
Flexural Strength 55.0 MPa
@Strain 3.5 %
7980 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 2.00 GPa290 ksiISO 178
Poissons Ratio 0.400.40
Charpy Impact, Notched  0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C66.7 µin/in-°FISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 136 °C277 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C172 °FISO 75-1/-2
Flame Spread 57.0 mm/min
@Thickness 2.00 mm
2.24 in/min
@Thickness 0.0787 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 °C392 °FOptimum, Extrusion
 195 - 205 °C383 - 401 °FRange, Extrusion
 200 - 210 °C392 - 410 °FRange, Injection
 205 °C401 °FOptimum, Injection
Mold Temperature 50.0 °C122 °FOptimum, Injection
 40.0 - 60.0 °C104 - 140 °FInjection
Drying Temperature 80.0 °C176 °FInjection
 75.0 - 85.0 °C167 - 185 °FExtrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourExtrusion, Dehumidified Dryer
 4.00 - 8.00 hour4.00 - 8.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.050 %<= 0.050 %Extrusion
 <= 0.050 %<= 0.050 %Injection
Hold Pressure 60.0 - 80.0 MPa8700 - 11600 psiInjection
 80.0 MPa11600 psiInjection
Annealing Temperature 160 °C320 °FOptional; 2 mm/min; Injection
 
Descriptive Properties
AdditivesRelease agent
Annealing time (min/mm)30Optional, Injection
Drying RecommendedyesInjection
Emissions (mg/kg)<2VDA 275
FMVSS ClassBISO 3795 (FMVSS 302)
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>POM-I<ISO 11469
PolymerPOM-I
Processing Hold Pressure Time (s/mm)7.5Injection
Resin IdentificationPOM-IISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
KEP Kepital® F10-52D Acetal Copolymer, UV-stabilized
Delrin Delrin® 300TE NC010 POM-I
Delrin Delrin® 150 NC010 POM
DuPont Mobility and Materials Delrin® II150E BK602 Acetal (POM)
Niagara LaSalle StressProof® Cold Finished Steel Bar

PDSX5108 / 197748

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.