MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
American Elements T-MITE™ Titanium Oxide Nanopowder
Categories: Ceramic; Oxide; Titanium Oxide

Material Notes: General Description

T-MITE™ powders and dispersions are recently developed inorganic titanium dioxide nanoparticles which impart special UV filtering and reflective properties to coatings and surfaces. T-MITE-A™ products are uncoated and hydrophilic. T-MITE-O™ products are coated with an organic silane (1-4%) and are hydrophobic. Particles are available in the size range of 10-200 nm.

Key Words: Formula: TiO2; CAS Number: 1317-80-2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.23 g/cc
Molecular Weight 79.9 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 1800 °C
 
Descriptive Properties
AppearanceWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech Rutile (TiO2) Fiber Optic Crystal
Titanium Dioxide, Rutile
CeramTec 192/193 Titania
Titanium Dioxide, Brookite
H.C. Starck Amperit® 745.8 Aluminum Oxide-Titanium Oxide 60-40 (Al2O3-TiO2)

EJAMER01 / 5484

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.