Dow SPECFLEX™ NC 638 Polyol
Categories:
Polymer
Material Notes:
SPECFLEX™ NC 632 polyol is a specialty capped polyol. Its high molecular weight and primary hydroxyl content make it well suited for high resilience, flexible molded foams. CAS# 009082-00-2 056449-05-9
Information provided by Dow
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.018
g/cc
1.018
g/cc
Viscosity Measure
1100
-
1400
cSt
1100
-
1400
cSt
ASTM D445
Maximum Moisture Content
0.060
0.060
wt% water; ASTM D203
ASTM Color
<= 30
<= 30
APHA; ASTM D4890
Chemical Properties
Metric
English
Comments
Total Acid Number
0.050
0.050
[mg KOH/g]; DOWM 100387-TE95A
Thermal Properties
Metric
English
Comments
Flash Point
>=
180
°C
>=
356
°F
ASTM D93
Descriptive Properties
Hydroxyl Number mg KOH/g
28.5 - 32.5
ASTM D4274
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Dow SPECFLEX™ NC 632 Polyol
Dow VORANOL™ 4701C Polyether Polyol
Dow VORANOL™ 4703 Polyether Polyol
Dow SPECFLEX™ NC 606 Polyol
Dow VORANOL™ 4240 Polyether Polyol
PDOW1426 / 30644
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.