MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lord Adhesives Thermoset™ TC-330 Thermally Conductive Silicone Grease
Categories: Fluid; Lubricant; Silicone Base; Silicone, Filled Grease

Material Notes: TC-330 is smooth, gray, microelectronics-grade, silicone-based, thermally conductive grease compound. It offers very high thermal conductivity, high temperature resistance, very low thermal resistance and easy dispensability. It is rated for use in applications where the continuous operating temperature is < 200°C and can withstand intermittent exposures up to 250-260°C. TC-330 has been designed for use in applications where device wattage’s can exceed 100 W and where the device may later need to be easily removed from the heat sink. It can be used with a variety of emerging and standard devices including microprocessors, DSPs, graphic accelerators, etc. packaged in flip-chip, PPGA, BGA, MicroBGA and other package types. TC-330 exhibits very low bleed and has been tested extensively in demanding environments. It has shown outstanding performance in reliability testing in microprocessor and other flip-chip applications. In addition, it has a significantly lower viscosity than competitive high thermal conductivity greases and can be easily dispensed even without going to special valve technology. It has been specially formulated for use in high throughput, automated dispensing equipment without the use of needle heating.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.92 g/cc
Loss On Ignition 0.14 %
@Temperature 100 °C,
Time 2.59e+6 sec
 1.0 %
@Temperature 300 °C,
Time 3600 sec
Viscosity 165000 cP
@Temperature 25.0 °C
10rpm
 250000 cP
@Temperature 25.0 °C
1rpm
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 7.21
@Frequency 1e+6 Hz,
Temperature 25.0 °C
ASTM D150
 7.4
@Frequency 100000 Hz,
Temperature 25.0 °C
ASTM D150
 7.62
@Frequency 10000 Hz,
Temperature 25.0 °C
ASTM D150
Dissipation Factor 0.0189
@Frequency 100000 Hz,
Temperature 25.0 °C
ASTM D150
 0.0215
@Frequency 1e+6 Hz,
Temperature 25.0 °C
ASTM D150
 0.0257
@Frequency 10000 Hz,
Temperature 25.0 °C
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 5.00 °C
 
Descriptive Properties
AppearanceGray
Thixotropic Index3.6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lord Adhesives Thermoset™ TC-350 Thermally Conductive Silicone Grease
NuSil G-9000 Silicone Grease
NuSil G-9020 Silicone Grease
DuPont MOLYKOTE® AS-828 Silicone Grease
NuSil G-9340 Silicone Grease

PLORD031 / 86039

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.