MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 1799 x 117570 A Modified Polyphenylene Oxide (PPO), Electrically Conductive - Flame Retardant
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.085 g/ccASTM D 792
Linear Mold Shrinkage 0.00080 - 0.0015 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 10000 psiASTM D 638
Elongation at Break 0.90 %ASTM D 638
Tensile Modulus 1500 ksiASTM D 638
Flexural Strength 14000 psiASTM D 790
Flexural Modulus 1200 ksiASTM D 790
Izod Impact, Notched 1.00 ft-lb/in
@Thickness 3.17 mm
D 256
Izod Impact, Unnotched 3.00 ft-lb/in
@Thickness 3.17 mm
ASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1e+05ASTM D 257
Surface Resistance <= 1.00e+6 ohmESD STM11.11
Surface Resistivity per Square <= 1.00e+7 ohmASTM D 257
Static Decay <= 2.0 secFTMS101C; 4046.1
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.59 mm
 V-2
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 480 - 550 °F
Mold Temperature 150 - 200 °F
Drying Temperature 200 °F
Dry Time 2 hour
Moisture Content 0.10 %
Dew Point 0.000 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 1701 Modified Polyphenylene Oxide (PPO), Glass Fiber
RTP Company RTP 1700  Modified Polyphenylene Oxide (PPO) Base Resin
RTP Company RTP 1700 FR Modified Polyphenylene Oxide (PPO), Flame Retardant - Halogen Free
RTP Company RTP 1700 GB 20 Z  Modified Polyphenylene Oxide (PPO) Glass Bead 20% - FDA Type
RTP Company RTP 1701 FR Modified Polyphenylene Oxide (PPO), Glass Fiber - Flame Retardant - Halogen Free

PQZWA11018 / 90570

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.