MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Phenolic, Novolac, Cellulose Filled
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Cellulose Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 - 1.60 g/ccAverage value: 1.34 g/cc Grade Count:29
Water Absorption 0.0800 - 1.90 %Average value: 0.822 % Grade Count:11
Linear Mold Shrinkage 0.00200 - 0.00400 cm/cmAverage value: 0.00294 cm/cm Grade Count:8
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 70.0 - 115Average value: 89.9 Grade Count:8
Tensile Strength, Ultimate 38.0 - 120 MPaAverage value: 64.1 MPa Grade Count:20
Flexural Yield Strength 55.0 - 175 MPaAverage value: 92.8 MPa Grade Count:28
Flexural Modulus 4.80 - 14.0 GPaAverage value: 7.84 GPa Grade Count:19
Compressive Yield Strength 70.0 - 350 MPaAverage value: 185 MPa Grade Count:28
Shear Strength 10.0 - 20.0 MPaAverage value: 15.0 MPa Grade Count:8
Izod Impact, Notched 0.315 - 0.683 J/cmAverage value: 0.512 J/cm Grade Count:10
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 100000 - 1.00e+10 ohmAverage value: 9.46e+8 ohm Grade Count:14
Dielectric Constant 5.50 - 6.00Average value: 5.67 Grade Count:6
Dielectric Strength 1.00 - 14.6 kV/mmAverage value: 6.99 kV/mm Grade Count:10
Dielectric Breakdown >= 20000 V
@Temperature 90.0 - 90.0 °C
Average value: 23300 V Grade Count:6
 >= 10000 V
@Temperature 90.0 - 90.0 °C
Average value: 23300 V Grade Count:8
 >= 10000 V
@Time 20.0 - 60.0 sec
Average value: 23300 V Grade Count:8
Dissipation Factor 0.0500 - 0.0550Average value: 0.0517 Grade Count:6
Arc Resistance 60.0 - 150 secAverage value: 101 sec Grade Count:8
Comparative Tracking Index 100 VAverage value: 100 V Grade Count:8
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 - 47.0 µm/m-°CAverage value: 32.1 µm/m-°C Grade Count:7
CTE, linear, Transverse to Flow 52.0 - 69.0 µm/m-°CAverage value: 58.0 µm/m-°C Grade Count:3
Thermal Conductivity 0.410 - 0.580 W/m-KAverage value: 0.522 W/m-K Grade Count:4
Maximum Service Temperature, Air 150 °CAverage value: 150 °C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 165 - 282 °CAverage value: 201 °C Grade Count:11
Flammability, UL94 HB - V-0Grade Count:9
 
Processing PropertiesOriginal ValueComments
Mold Temperature 150 - 180 °CAverage value: 166 °C Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled
Sumitomo Bakelite North America RX® 448 Cellulose Reinforced Phenolic Novolac
G-3 Fiberglass Phenolic Laminate Sheet
Overview of materials for Phenolic, Novolac, Glass Filled
LE Phenolic Laminate

O2736 / 78099

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.