MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Industeel CLC 17.13.5 LN Modified 317LN Mo 4% Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T S30000 Series Stainless Steel

Material Notes: Description: CLC 17-13-5LN (317LNM) is a Nitrogen alloyed austenitic stainless steel with a high Molybdenum addition (=4%). Alloy CLC 17-13-5LN (317LNM) exhibits austenitic microstructure free of deleterious carbide precipitations in grain boundaries. The grade contains some residual ferrite (=2%) after solution annealing (1100 - 1150°C / 2012 - 2102°F) and water quenching. Its low carbon content avoids the intergranular corrosion, even on welded pieces without an ulterior water quenching. The high Molybdenum content gives this steel a higher resistance to corrosion in chloride containing environments than standard grades (CLC17-12-2L / 316L). Nitrogen additions and a low silicon content have a stabilizing effect on austenitic structure reducing, therefore, precipitation of inter-metallic phases during welding. Nitrogen addition also increases the yield strength compared to CLC 18-15-4L (317L). Its main properties are : high ductility, easy weldability and high corrosion resistance. The main applications are chemical and petrochemical applications, pollution control equipments and chemical tankers.

Information provided by manufacturer.

Key Words: EURONORM 1.4439 X2CrNiMoN17.13.5, AFNOR Z3CND 18-14 05Az, DIN W 1.4439, ASTM A240 TP 317LNM, UNS S31725, UNS S31726
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 590 MPa
Tensile Strength, Yield >= 285 MPa
@Strain 0.2 %
 >= 315 MPa
@Strain 1 %
Elongation at Break >= 40 %
Modulus of Elasticity 200 GPa
@Temperature 20.0 - 100 °C
Poissons Ratio 0.299Calculated
Shear Modulus 77.0 GPa
@Temperature 20.0 - 100 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000800 ohm-cm
@Temperature 20.0 - 100 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 - 100 °C
 16.5 µm/m-°C
@Temperature 20.0 - 200 °C
 17.0 µm/m-°C
@Temperature 20.0 - 300 °C
 18.0 µm/m-°C
@Temperature 20.0 - 500 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 - 100 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.020 %
Chromium, Cr 18.2 %
Iron, Fe 63.43 %As remainder
Molybdenum, Mo 4.2 %
Nickel, Ni 14 %
Nitrogen, N 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 60% Cold Rolled (UNS S30403)
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel
Steels, General Properties
AISI 4130 Steel, annealed at 865°C (1585°F), furnace cooled 11°C (20°F)/hour to 680°C (1255°F), air cooled, 25 mm (1 in.) round
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel

NINDUST09 / 17547

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.