MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Texin® 985 U Thermoplastic Polyurethanes (TPU)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Texin 985U resin is an aromatic polyether-based thermoplastic polyurethane with a Shore hardness of approximately 85A. It can be processed by injection molding, extrusion, or blow molding.

Properties / Applications: Texin 985U resin offers good clarity and outstanding abrasion resistance, impact strength, toughness, and flexibility. It is stabilized against degradation due to heat and UV exposure. It also exhibits excellent hydrolytic stability, as well as excellent microbial resistance. Typical applications include belting, hose, cable jackets, hose jackets, seals and gaskets, athletic soles, casters, mine screens, tubing, film, and extruded profiles. Texin 985U natural color resin is listed under NSF Standard 61 for use in potable water applications.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0080 cm/cm
@Thickness 2.54 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.54 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85ASTM D2240
Tensile Strength at Break 38.6 MPaASTM D412
Tensile Stress at Strain 4.80 MPa
@Strain 50 %
ASTM D412
 5.50 MPa
@Strain 100 %
ASTM D412
 9.70 MPa
@Strain 300 %
ASTM D412
Elongation at Break 590 %ASTM D412
Flexural Modulus 26.9 MPa
@Thickness 584 mm
ASTM D790
 59.0 MPa
@Thickness -762 mm
ASTM D790
Compressive Strength 0.300 MPa2% Deflection; ASTM D 575
 1.00 MPa5% Deflection; ASTM D 575
 2.10 MPa10% Deflection; ASTM D 575
 3.10 MPa15% Deflection; ASTM D 575
 4.30 MPa20% Deflection; ASTM D 575
 5.50 MPa25% Deflection; ASTM D 575
 16.5 MPa50% Deflection; ASTM D 575
Resilience 45[%], Bayshore; ASTM D2632
Tear Strength 87.6 kN/mDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 30
@Load 1.00 kg
[mg] Loss, H-18; ASTM D3489
Compression Set 16 %
@Temperature 23.0 °C,
Time 79200 sec
postcured; ASTM D395-B
 19 %
@Temperature 23.0 °C,
Time 79200 sec
as molded; ASTM D395-B
 40 %
@Temperature 70.0 °C,
Time 79200 sec
postcured; ASTM D395-B
 80 %
@Temperature 70.0 °C,
Time 79200 sec
as molded; ASTM D395-B
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 80.0 °CRate A; ASTM D1525
Brittleness Temperature >= -68.0 °FASTM D746
Glass Transition Temp, Tg -46.0 °C
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 180 - 200 °CExtrusion
 182 - 199 °CInjection
Middle Barrel Temperature 180 - 205 °CExtrusion
 182 - 205 °CInjection
Front Barrel Temperature 180 - 210 °CExtrusion
 182 - 210 °CInjection
Nozzle Temperature 188 - 213 °CInjection
Adapter Temperature 180 - 210 °CExtrusion
Die Temperature 185 - 210 °CExtrusion
Melt Temperature 196 °CInjection
 190 - 205 °CExtrusion
Mold Temperature 16.0 - 38.0 °CInjection
Injection Pressure 6000 - 15000 psiInjection
Back Pressure <= 200 psiInjection
Cushion <= 0.125 inInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman AVALON® 90 ABR Thermoplastic Polyurethane
Huntsman AVALON® 95 AB Thermoplastic Polyurethane
Covestro Texin® 4210 Thermoplastic Polyurethanes (TPU)
Covestro Texin® 985 Thermoplastic Polyurethanes (TPU)
Covestro Texin® 4215 Thermoplastic Polyurethanes (TPU)

PCOVEST0984 / 202767

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.