MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain Rulon® 125 Bearing/Seal PTFE
Categories: Polymer; Thermoplastic

Material Notes: Rulon 125 is used primarily in applications that are not severe such as dryer drum slides and piston rings in pneumatic or hydraulic controls.

Information provided by distributor TriStar Plastics Corp.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.09 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60
Tensile Strength, Yield 1500 psi
Elongation at Break 60 %
Tensile Modulus 230000 psi
Flexural Modulus 200000 psi
Izod Impact, Notched 6.00 ft-lb/in
Coefficient of Friction, Dynamic 0.012Dry vs. Steel
Coefficient of Friction, Static 0.018Dry vs. Steel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm
Dielectric Constant 2.65
@Frequency 1e+6 Hz
Dielectric Strength 375 kV/inShort Term
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 4.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 550 °FContinuous
 600 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 225 °F
Minimum Service Temperature, Air -400 °FEmbrittlement Temp
Flammability, UL94 V-0
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Manifattura Cattaneo RULON® LR Polytetrafluoroethylene
Saint-Gobain Rulon® 1337 Bearing/Seal PTFE
Saint-Gobain Rulon® DC1042 Bearing/Seal PTFE
Saint-Gobain Rulon® 954 Bearing/Seal PTFE
Manifattura Cattaneo RULON® W2 Polytetrafluoroethylene

PSTGQ992b / 170602

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.