MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EconCore ThermHex THPP80-FN Polypropylene Honeycomb Core Sheet
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: The ThermHex core is produced from a single sheet by a thermoforming, a folding and a bonding operation. ThermHex honeycombs have closed skin strips, allowing perfect bonding of skins onto the core. ThermHex technology enables the cost efficient production of honeycomb cores from a wide range of thermoplastic polymers with a large variation in cell size, density and thickness.

The 100% polypropylene (PP) ThermHex honeycomb boards are especially applicable to reusable plastic transportation boxes and solutions in the logistics sector, such us for example durable and hygienic plastic pallets. Layer pads, dividers, protection panels are complementary applications. Honeycomb panels are also used in promotional materials because the PP boards are printable.

The surface finish of ThermHex FN grades are a 50 µm polypropylene film plus 40 g/m² nonwoven polyester fleece. Standard dimensions are 1.2 m x 2.5 m.

Information provided by EconCore.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0800 - 0.0900 g/cc
Thickness 8000 - 10000 micronscell diameter 8.0 mm
 15000 - 28000 micronscell diameter 9.6 mm
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 1.20 MPaASTM D365-57
Compressive Modulus 0.0400 GPaASTM D365-57
Shear Modulus 0.00600 GPaLength; ASTM C273-61
 0.0150 GPaWidth; ASTM C273-61
Shear Strength 0.300 MPaLength; ASTM C273-61
 0.500 MPaWidth; ASTM C273-61
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0650 W/m-K
Maximum Service Temperature, Air 80.0 °C
 140 °CShort Term
Minimum Service Temperature, Air -30.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 °C
 140 °CShort Term

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EconCore ThermHex THPP60-FN Polypropylene Honeycomb Core Sheet
EconCore ThermHex THPP120-FN Polypropylene Honeycomb Core Sheet
3A Composites Core Materials AIREX® T92.80 Easy Processing Structural Foam
DIAB Divinycell® PX 100 Sandwich Core Material
Poly-u-Mac Air-Comb PP8-80 Polypropylene Honeycomb Material

PECONC991 / 192645

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.