MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Impet® 2700 GV1/30 PET, 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 30% Glass Reinforced

Material Notes: 30% glass filled Polyethylene terephthalate (PET) with high flowability, excellent gloss, high modulus, and high heat deflection temperature.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/ccISO 1183
Moisture Absorption 0.150 %23°C/50%RH; ISO 62
Viscosity Test 50 cm³/gISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0090 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 123ISO 2039-2
Tensile Strength at Break 168 MPa5mm/min; ISO 527-2/1A
Elongation at Break 2.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 11500 MPa50mm/min; ISO 527-2/1A
Flexural Strength 225 MPaISO 178
Flexural Modulus 11100 MPaISO 178
Izod Impact, Notched (ISO) 7.30 kJ/m²ISO 180/1A
Charpy Impact Unnotched 28.0 kJ/m²ISO 179/1eU
 28.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 8.80 kJ/m²ISO 179/1eA
 8.80 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+16 ohm-cmIEC 60093
Surface Resistance 3.00e+15 ohmIEC 60093
Dielectric Constant 4.2
@Frequency 1e+6 Hz
IEC 60250
 4.8
@Frequency 100 Hz
IEC 60250
Dielectric Strength 33.0 kV/mmIEC 60243-1
Dissipation Factor 0.013
@Frequency 100 Hz
IEC 60250
 0.018
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 170 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 21.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 64.0 µm/m-°CISO 11359-2
Melting Point 251 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 252 °CISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 225 °CISO 75-1, -2
Deflection Temperature at 8.0 MPa 135 °CISO 75-1, -2
Vicat Softening Point 260 °CISO 306
Glass Transition Temp, Tg 80.0 °CISO 11357-1,-2,-3
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 0.800 mm
Oxygen Index 25 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Processing Temperature 135 - 145 °Ccavity
 270 - 290 °Chot runner
Feed Temperature 40.0 - 60.0 °C
Zone 1 260 - 270 °C
Zone 2 270 - 280 °C
Zone 3 280 - 290 °C
Zone 4 280 - 290 °C
Die Temperature 270 - 290 °C
Melt Temperature 270 - 290 °C
Drying Temperature 120 - 140 °C
Dry Time 2.00 - 4.00 hour
Moisture Content <= 0.010 %
Screw Speed 50 rpm
@Diameter 55.0 mm
 65 rpm
@Diameter 40.0 mm
 80 rpm
@Diameter 25.0 mm
 
Descriptive Properties
Injection moldingYes
Injection speedfast
pvT (Generic Grade reference)PET-09-110, GF30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grivory® HT2V-3X V0 black 9021 PA6T/66-GF30
Celanese Hostaform® C 9021 GV1/30 POM, 30% Glass Reinforced
Celanese Impet® 2700 GV1/45 (Europe) PET, 45% Glass Reinforced
LATI Latan 13 G/30 POM, 30% Glass Fiber Reinforced
Celanese Hostaform® C 27021 GV3/30 POM, 30% Glass Reinforced

PHCQ441 / 178896

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.