MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Silres® BS OH 100 Silicone Masonry Water Repellent
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: SILRES® BS OH 100 is a solventless, ready-to-use product for the consolidation of construction materials.

Special features:

  • one-pack system - easy processing
  • low-molecular weight - optimum penetration
  • tack-free drying - therefore no dirt attraction
  • no by-products that are damaging to the building material
  • the binder formed is mineral - therefore resembling the building material
  • the binder formed is acid-resistant-therefore resistant to rainwater
  • pores are not sealed - therefore the treated building material maintains its water vapour permeability
Mode of action SILRES® BS OH 100 is based on ethyl silicate. When applied, it penetrates through the capillaries deep into the construction material. The neutral catalyst promotes the reaction between ethyl silicate and water from atmospheric humidity or the moisture in the capillary pores. A glass-like silica gel binder (SiO2 .aq.) is formed. The ethanol by product evaporates. Under standard conditions (20°C / 50% r. h. ), final hardness is reached after two weeks, i. e. when most of the ethyl silicate has been converted to silica gel. The product does not contain any hydrophobic additives such as silanes or siloxanes. Before the reaction is complete, the treated surface may show slight beading, though this does not mean that it is water repellent.

Application: The main application of the product is to restore weather-damaged natural stone, stucco or frescos. It may also be used to treat other construction materials such as brick or terracotta. Any absorbent mineral construction material can be treated with SILRES® BS OH 100. By saturation with the product, their original strength and porosity can be practically restored.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.997 g/ccDIN 51757
 
Thermal PropertiesOriginal ValueComments
Flash Point 40.0 °CISO 2719
Ignition Temperature 230 °CDIN 51794
 
Descriptive Properties
Appearancecolorless to yellowish
Content (%)100Ethyl silicate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Dehesive® 944 Silicone Release Coating
Wacker Dehesive® SFX 250 Silicone Release Coating
Wacker Dehesive® SF 500 Silicone Release Coating
Wacker Dehesive® EM 490 Silicone Release Coating
Wacker Dehesive® EM 426 Silicone Release Coating

PWACK9563 / 205092

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.