MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Apec® DP9-9354T High-Heat Polycarbonate, Transparent, Flame-Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Information provided by Bayer Corporation, Plastics Division

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccASTM D792
Water Absorption 0.20 %24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0080 - 0.0090 cm/cmASTM D955
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 330 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 62.0 MPaASTM D638
Tensile Strength, Yield 66.0 MPaASTM D638
Elongation at Break 50 %ASTM D638
Elongation at Yield 6.0 %ASTM D638
Tensile Modulus 2.20 GPaASTM D638
Flexural Yield Strength 86.0 MPaASTM D790
Flexural Modulus 2.28 GPaASTM D790
Izod Impact, Notched 1.00 J/cm
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched NBASTM D256
 NB
@Temperature -40.0 °C
ASTM D256
Impact Test 58.0 J
@Thickness 3.20 mm
Instrumented Impact, Total Energy; 3.2 mm thick, 15 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+16 ohmASTM D257
Dielectric Constant 2.9
@Frequency 60 Hz
ASTM D150
 2.9
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength >= 16.0 kV/mm
@Thickness 3.17 mm
ASTM D149
Dissipation Factor 0.0010
@Frequency 60 Hz
ASTM D150
 0.010
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 60 - 120 sec
@Thickness 3.00 mm
UL Rating PLC 6 (60-120 sec)
Comparative Tracking Index >= 600 V
@Thickness 3.00 mm
UL Rating PLC 0 (>600 V)
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness 1.50 mm
UL Rating PLC 2 (30-60 sec)
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.50 mm
UL Rating PLC 0 (>120 arcs)
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min
@Thickness 3.00 mm
UL Rating PLC 2 (25.4-80 mm/min.)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.210 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 174 °C
@Thickness 3.20 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 162 °C
@Thickness 3.17 mm
ASTM D648
Vicat Softening Point 185 °CRate B; ASTM D1525
Flammability, UL94 V-0
@Thickness 3.00 mm
 V-0
@Thickness 3.00 mm
Oxygen Index 35 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.573ASTM D542
Haze 2.0 %
@Thickness 3.17 mm
ASTM D1003
Transmission, Visible 87 %
@Thickness 3.20 mm
ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 6555 Polycarbonate, Injection Grade
Covestro Apec® DP9-9373 High-Heat Polycarbonate, General Purpose, UV-Stabilized
Covestro Makrolon® 6717 Polycarbonate, Flame Retardant Grade
Covestro Makrolon® 6870 Polycarbonate
Covestro Makrolon® 6455 Polycarbonate, Flame Retardant Grade

PB1A08 / 26390

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.