MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Exceed™ 2018EB Metallocene Polyethylene Resin (European Grade)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Exceed 2018EB is a metallocene ethylene-hexene copolymer. The higher melt index makes this polymer ideally suited for blending into LDPE rich films.

Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: 2500 ppm
  • Slip: 750 ppm
  • Processing Aid: Yes
  • Thermal Stabilizer: Yes
Applications:
  • Bag in Box
  • Blown Film
  • Bread Bags
  • Food packaging
  • Freezer Film
  • Garment Film
  • General Packaging
  • Industrial Packaging
  • Lamination Film
  • Mulch Film
  • Multilayer Packaging Film
  • Packaging Films
  • Thin Gauged Consumer Bags

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccExxonMobil method
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 2500 ppm
Slip Level 750 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 480 %ASTM D882
Film Elongation at Break, TD 520 %ASTM D882
Elmendorf Tear Strength MD 280 gASTM D1922
Elmendorf Tear Strength TD 500 gASTM D1922
Dart Drop Test 750 gASTM D1709
Film Tensile Strength at Break, MD 5800 psiASTM D882
Film Tensile Strength at Break, TD 4400 psiASTM D882
1% Secant Modulus, MD 25000 psiASTM D882
1% Secant Modulus, TD 25000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 244 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesOriginal ValueComments
Haze 6.0 %ASTM D1003
Gloss 11 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force14 lbfExxonMobil Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin
ExxonMobil Exceed™ 2018CA Metallocene Polyethylene Resin (European Grade)
Dow Engage® 8150 Polyolefin Elastomer
ExxonMobil Exceed™ 1018EB Metallocene Polyethylene Resin (European Grade)
Dow Engage® 8200 Polyolefin Elastomer

PEX99051 / 175287

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.