MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Nylon 66, Unreinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.02 - 2.70 g/ccAverage value: 1.17 g/cc Grade Count:517
Water Absorption 0.300 - 9.50 %Average value: 3.51 % Grade Count:226
Moisture Absorption at Equilibrium 0.170 - 8.50 %Average value: 2.47 % Grade Count:168
 2.90 - 3.10 %
@Temperature 70.0 - 70.0 °C
Average value: 3.00 % Grade Count:6
Water Absorption at Saturation 1.70 - 9.00 %Average value: 6.44 % Grade Count:99
Viscosity 2.48 - 50.0 cPAverage value: 9.44 cP Grade Count:7
 13.0 - 700000 cP
@Temperature 200 - 300 °C
Average value: 122000 cP Grade Count:12
 13.0 - 700000 cP
@Shear Rate 30.0 - 10000 1/s
Average value: 122000 cP Grade Count:12
Viscosity Test 115 - 160 cm³/gAverage value: 141 cm³/g Grade Count:7
Viscosity Number 140 - 330 cm³/gAverage value: 199 cm³/g Grade Count:15
Maximum Moisture Content 0.0200 - 0.200Average value: 0.139 Grade Count:29
 0.200 - 0.200
@Temperature 120 - 120 °C
Average value: 0.200 Grade Count:1
 0.200 - 0.200
@Time 299 - 299 sec
Average value: 0.200 Grade Count:1
Linear Mold Shrinkage 0.00100 - 0.0310 cm/cmAverage value: 0.0139 cm/cm Grade Count:337
Linear Mold Shrinkage, Transverse 0.00160 - 0.0740 cm/cmAverage value: 0.0157 cm/cm Grade Count:156
Melt Flow 2.00 - 180 g/10 minAverage value: 52.5 g/10 min Grade Count:56
Spiral Flow 104 - 105 cmAverage value: 104 cm Grade Count:4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 55.0 - 90.0Average value: 75.8 Grade Count:31
Hardness, Rockwell R 78.0 - 121Average value: 114 Grade Count:82
 97.0 - 97.0
@Temperature 80.0 - 80.0 °C
Average value: 97.0 Grade Count:3
Hardness, Shore D 76.0 - 88.0Average value: 82.2 Grade Count:15
Ball Indentation Hardness 70.0 - 180 MPaAverage value: 137 MPa Grade Count:12
Tensile Strength, Ultimate 7.52 - 260 MPaAverage value: 81.2 MPa Grade Count:274
 28.0 - 116 MPa
@Temperature -40.0 - 80.0 °C
Average value: 76.8 MPa Grade Count:6
Tensile Strength, Yield 10.0 - 98.0 MPaAverage value: 72.1 MPa Grade Count:298
 44.8159 - 44.8159 MPa
@Temperature 77.0 - 77.0 °C
Average value: 44.8 MPa Grade Count:1
Elongation at Break 0.000 - 300 %Average value: 47.6 % Grade Count:436
 >= 100 %
@Temperature 60.0 - 150 °C
Average value: 100 % Grade Count:1
Elongation at Yield 1.50 - 210 %Average value: 13.9 % Grade Count:220
 30.0 - 30.0 %
@Temperature 76.7 - 76.7 °C
Average value: 30.0 % Grade Count:1
Modulus of Elasticity 0.600 - 25.0 GPaAverage value: 3.47 GPa Grade Count:346
 0.350 - 1.90 GPa
@Temperature 60.0 - 150 °C
Average value: 0.850 GPa Grade Count:1
Flexural Yield Strength 11.0 - 350 MPaAverage value: 102 MPa Grade Count:361
 29.9922 - 140 MPa
@Temperature -40.0 - 90.0 °C
Average value: 85.3 MPa Grade Count:7
Flexural Modulus 0.600 - 18.5 GPaAverage value: 3.01 GPa Grade Count:413
 0.500 - 4.30 GPa
@Temperature -40.0 - 90.0 °C
Average value: 2.27 GPa Grade Count:7
Flexural Strain at Break 5.50 - 9.00 %Average value: 7.38 % Grade Count:12
Compressive Yield Strength 7.00 - 100 MPaAverage value: 57.6 MPa Grade Count:14
Poissons Ratio 0.380 - 0.450Average value: 0.400 Grade Count:22
Shear Strength 50.0 - 80.0 MPaAverage value: 70.3 MPa Grade Count:9
Izod Impact, Notched 0.300 - 8.54 J/cmAverage value: 1.04 J/cm Grade Count:154
 0.240 - 0.480 J/cm
@Temperature -40.0 - -20.0 °C
Average value: 0.385 J/cm Grade Count:8
 0.490332 - 0.490332 J/cm
@Temperature 3.20 - 3.20 °C
Average value: 0.385 J/cm Grade Count:1
 0.490332 - 0.490332 J/cm
@Thickness 23.0 - 23.0 mm
Average value: 0.385 J/cm Grade Count:1
Izod Impact, Unnotched 0.0510 J/cm - NBAverage value: 5.01 J/cm Grade Count:20
Izod Impact, Notched (ISO) 3.00 - 21000 kJ/m²Average value: 13.4 kJ/m² Grade Count:192
 3.00 - 50.0 kJ/m²
@Temperature -40.0 - -20.0 °C
Average value: 7.72 kJ/m² Grade Count:62
Izod Impact, Unnotched (ISO) 35.7 - 21000 kJ/m²Average value: 79.2 kJ/m² Grade Count:29
 55.0 kJ/m² - NB
@Temperature -30.0 - -30.0 °C
Average value: 88.8 kJ/m² Grade Count:12
Charpy Impact Unnotched 1.00 J/cm² - NBAverage value: 7.03 J/cm² Grade Count:268
 0.400 J/cm² - NB
@Temperature -40.0 - -5.00 °C
Average value: 7.36 J/cm² Grade Count:139
Charpy Impact, Notched 0.100 - 2100 J/cm²Average value: 1.34 J/cm² Grade Count:292
 0.100 J/cm² - NB
@Temperature -40.0 - -5.00 °C
Average value: 0.827 J/cm² Grade Count:140
Gardner Impact 6.78 - 22.6 JAverage value: 13.6 J Grade Count:3
Puncture Energy 13.1 - 50.0 JAverage value: 27.7 J Grade Count:4
 5.10 - 60.0 J
@Temperature -30.0 - -30.0 °C
Average value: 20.4 J Grade Count:3
Coefficient of Friction 0.100 - 0.420Average value: 0.246 Grade Count:13
Coefficient of Friction, Static 0.172 - 0.200Average value: 0.184 Grade Count:3
Tensile Creep Modulus, 1 hour 1000 - 3400 MPaAverage value: 2760 MPa Grade Count:9
Tensile Creep Modulus, 1000 hours 450 - 980 MPaAverage value: 676 MPa Grade Count:10
K (wear) Factor 24.2 - 403 x 10-8 mm³/N-MAverage value: 308 x 10-8 mm³/N-M Grade Count:4
Taber Abrasion, mg/1000 Cycles 4.00 - 8.00Average value: 6.75 Grade Count:12
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 4000 - 1.00e+17 ohm-cmAverage value: 1.21e+15 ohm-cm Grade Count:196
Surface Resistance 100 - 1.00e+15 ohmAverage value: 1.19e+14 ohm Grade Count:116
Dielectric Constant 1.60 - 15.0Average value: 4.31 Grade Count:128
Dielectric Strength 9.84 - 120 kV/mmAverage value: 31.5 kV/mm Grade Count:153
Dissipation Factor 0.000200 - 0.320Average value: 0.0616 Grade Count:82
Dielectric Loss Index 0.0150 - 0.200Average value: 0.0989 Grade Count:11
Arc Resistance 60.0 - 240 secAverage value: 144 sec Grade Count:29
Comparative Tracking Index 350 - 650 VAverage value: 587 V Grade Count:150
Hot Wire Ignition, HWI 7.00 - 60.0 secAverage value: 22.2 sec Grade Count:18
High Amp Arc Ignition, HAI 60.0 - 120 arcsAverage value: 117 arcs Grade Count:18
High Voltage Arc-Tracking Rate, HVTR 0.000 - 50.0 mm/minAverage value: 6.92 mm/min Grade Count:17
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 - 130 µm/m-°CAverage value: 81.2 µm/m-°C Grade Count:107
 71.0 - 100 µm/m-°C
@Temperature 35.0 - 55.0 °C
Average value: 95.7 µm/m-°C Grade Count:18
 71.0 - 100 µm/m-°C
@Thickness 2.00 - 2.00 mm
Average value: 95.7 µm/m-°C Grade Count:18
CTE, linear, Transverse to Flow 67.0 - 130 µm/m-°CAverage value: 95.7 µm/m-°C Grade Count:48
Specific Heat Capacity 1.45 - 2.10 J/g-°CAverage value: 1.72 J/g-°C Grade Count:29
Thermal Conductivity 0.200 - 11.0 W/m-KAverage value: 1.06 W/m-K Grade Count:45
Melting Point 197 - 270 °CAverage value: 258 °C Grade Count:356
Maximum Service Temperature, Air 70.0 - 249 °CAverage value: 136 °C Grade Count:60
Hot Ball Pressure Test 125 - 165 °CAverage value: 158 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 70.0 - 260 °CAverage value: 211 °C Grade Count:284
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 250 °CAverage value: 91.6 °C Grade Count:395
Deflection Temperature at 8.0 MPa 50.0 - 60.0 °CAverage value: 53.3 °C Grade Count:3
Vicat Softening Point 23.0 - 255 °CAverage value: 233 °C Grade Count:96
Minimum Service Temperature, Air -40.0 - -20.0 °CAverage value: -30.0 °C Grade Count:12
Glass Transition Temp, Tg 5.00 - 72.0 °CAverage value: 39.1 °C Grade Count:10
Decomposition Temperature 300 - 310 °CAverage value: 308 °C Grade Count:10
UL RTI, Electrical 65.0 - 140 °CAverage value: 124 °C Grade Count:23
UL RTI, Mechanical with Impact 65.0 - 110 °CAverage value: 77.8 °C Grade Count:23
UL RTI, Mechanical without Impact 65.0 - 125 °CAverage value: 86.2 °C Grade Count:23
Flammability, UL94 HB - V-0Grade Count:234
Flame Spread 0.000 - 30.0 mm/minAverage value: 10.0 mm/min Grade Count:6
Oxygen Index 20.0 - 34.0 %Average value: 26.1 % Grade Count:48
Glow Wire Test 649 - 960 °CAverage value: 837 °C Grade Count:58
Ignition Temperature 400 °CAverage value: 400 °C Grade Count:10
 
Optical PropertiesOriginal ValueComments
Yellow Index -10.0 - 8.00 %Average value: -4.00 % Grade Count:14
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 310 °CAverage value: 258 °C Grade Count:68
Nozzle Temperature 250 - 310 °CAverage value: 285 °C Grade Count:75
Die Temperature 270 - 295 °CAverage value: 283 °C Grade Count:6
Melt Temperature 209 - 320 °CAverage value: 279 °C Grade Count:250
Mold Temperature 20.0 - 150 °CAverage value: 75.6 °C Grade Count:263
Drying Temperature 48.9 - 140 °CAverage value: 81.5 °C Grade Count:223
Moisture Content 0.0200 - 0.500 %Average value: 0.158 % Grade Count:73
Dew Point -40.0 - -17.8 °CAverage value: -22.2 °C Grade Count:5
Injection Pressure 3.45 - 138 MPaAverage value: 79.7 MPa Grade Count:45
Vent Depth 0.000762 cmAverage value: 0.000762 cm Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 46, Unreinforced
Overview of materials for Nylon 66/6
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded

O2500 / 77999

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.