MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil C4LL 20025.17 Linear Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: ExxonMobil™ C4LL 20025.17 is a narrow molecular weight butene copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in freezer applications for food packaging

Availability: Latin America and North America

Additive: Antiblock: No; Slip: No; Thermal Stabilizer: Yes

Applications:

  • Closures and Dispensers
  • Housewares
  • Protective Caps

Information provided by ExxonMobil

Key Words: ExxonMobil ™ LLDPE LL 6100.17
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.925 g/ccExxonMobil method
ESCR 10% Igepal® 110 hourF50; ASTM D1693B
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 1900 psiASTM D638
Elongation at Break 360 %ASTM D638
Flexural Modulus 60000 psi
@Strain 2 %
Secant; ASTM D638
Flexural Modulus, 1% Secant 69000 psiASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 255 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 87.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil LL 6100.17 Injection Molding Resin
ExxonMobil Escorene® LL-6101 LLDPE, Injection Grade
ExxonMobil LLDPE LLP 8360.29 Linear Low Density Polyethylene Resin
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
DuPont Teijin Films Mylar® LB Polyester Film, 92 Gauge (23 µm)

PEX99168 / 175404

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.