MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-THERM 1641 Thermally Conductive Silicone
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Thermally Conductive Silicone Compound. This compound is a one-component thermally conductive electrically insulating silicone based RTV adhesive/sealant/potting compound.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.10 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 78ASTM D2240
Elongation at Break 30 %ASTM D412
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmASTM D257
Dielectric Constant 3.9
@Frequency 100000 Hz
ASTM D150
 4.1
@Frequency 100 Hz
ASTM D150
Dielectric Strength 500 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 112 µm/m-°C
@Temperature 24.0 - 105 °C
Thermal Conductivity 0.900 W/m-KASTM D5470
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -70.0 °C
Brittleness Temperature -75.0 °C
 
Processing PropertiesOriginal ValueComments
Extrusion Rate 1.30 g/min14 ga needle/60 psi
Cure Time 48.0 hour
@Temperature 24.0 °C
50% RH
Pot Life 30 min
Shelf Life 6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow TC-5121 Thermally Conductive Compound
Dow TC-5688 Thermally Conductive Compound
Parker Chomerics CHO-THERM 1642 Thermally Conductive Silicone
Celanese CoolPoly® E4501 Thermally Conductive Polycarbonate
Celanese CoolPoly® E4301 Thermally Conductive Polybutylene Terephthalate

PCHOME175 / 28397

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.