MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
DSM Somos® ProtoGen™ 18420 Epoxy Resin for Stereolithography, UV & Thermal Postcure
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoset; Epoxy

Material Notes: Description: DSM’s Somos® ProtoGen 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. Somos® ProtoGen resins are the first stereolithography resins to demonstrate different material properties based on machine exposure control. Based on Somos® Oxetane™ chemistry, Somos® ProtoGen 18420 offers superior chemical resistance, a wide processing latitude and excellent tolerance to a broad range of temperatures and humidity, both during and after the build.

Application: This high-temperature resistant, ABS-like photopolymer is used in solid imaging processes, like stereolithography, to build three-dimensional parts. Somos® ProtoGen 18420 provides considerable processing latitude and is ideal for the medical, electronic, aerospace and automotive markets that demand accurate RTV patterns, durable concept models, highly accurate and humidity & temperature resistant parts.

Information Provided by DSM Desotech Inc.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. North American leaders in producing short turnaround Rapid Prototyping and short run manufacturing solutions using all major 3D printing systems including SLA 3D printing technology. Free 3D printing quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.16 g/cc
@Temperature 25.0 °C
Water Absorption 0.61 %ASTM D570-98
Viscosity 350 cP
@Temperature 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 86 - 87ASTM D2240
Tensile Strength, Yield 66.1 - 68.1 MPaASTM D638M
Elongation at Break 6.0 - 9.0 %ASTM D638M
Tensile Modulus 2880 - 2960 MPaASTM D638M
Flexural Strength 84.9 - 87.7 MPaASTM D790M
Flexural Modulus 2280 - 2340 MPaASTM D790M
Poissons Ratio 0.40 - 0.42ASTM D638M
Izod Impact, Notched 15.0 - 18.0 J/cmASTM D256A
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.9 - 3.0
@Frequency 1e+6 Hz
ASTM D150-98
 3.1 - 3.2
@Frequency 1000 Hz
ASTM D150-98
 3.1 - 3.3
@Frequency 60.0 Hz
ASTM D150-98
Dielectric Strength 13.8 - 14.1 kV/mmASTM D149-97a
 
Thermal PropertiesOriginal ValueComments
CTE, linear 67.3 - 68.2 µm/m-°C
@Temperature -40.0 - 0.000 °C
ASTM E831-00
 82.2 - 86.4 µm/m-°C
@Temperature 0.000 - 50.0 °C
ASTM E831-00
 110.4 - 116 µm/m-°C
@Temperature 50.0 - 100 °C
ASTM E831-00
 152.7 - 163.2 µm/m-°C
@Temperature 100 - 150 °C
ASTM E831-00
Deflection Temperature at 0.46 MPa (66 psi) 93.0 - 98.0 °CASTM D648-98c
Deflection Temperature at 1.8 MPa (264 psi) 74.0 - 78.0 °CASTM D648-98c
Glass Transition Temp, Tg 78.0 - 96.0 °CASTM E1545-00
 
Descriptive Properties
AppearanceWhite
Dp (mm)0.11Slope of cure-depth vs. ln(E) curve
E10 (mJ/cm2)67.6Exposure that gives 0.254mm thickness
Ec (mJ/cm2)6.73Critical exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DSM Somos® ProtoGen™ 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC -2
DSM Somos® ProtoGen™ 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC +3
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
DSM Somos® NanoTool™ Resin for Stereolithography, UV & Thermal Postcure

PDSMT008 / 93528

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.